Linsy aluminum wire is produced through an integrated, high-speed process ensuring optimal electrical and mechanical properties. The process begins with continuous casting from the Melting Furnace to form a large rod. This rod is then reduced in diameter via Drawing Machines and conditioned in Annealing Furnaces. The wire is finished by Strandinginto final conductors, ensuring excellent conductivity and dimensional accuracy for all applications.







高純度アルミニウムと合金元素は、 溶解炉. 溶融金属はその後、固体の円筒形に凝固する。 ラウンドインゴット 使用して 連続鋳造設備. これにより、材料の組成が均一になり、その後の加工に不可欠な緻密で細粒の構造が確保されます。.
The as-rolled wire rod is fed into a high-speed Wire Drawing Machine. The rod is pulled through a series of successively smaller dies, reducing its diameter significantly while simultaneously increasing its mechanical strength through work hardening. This step is crucial for achieving the final gauge and strength.
Depending on the required temper (e.g., O temper for soft wire), the drawn wire undergoes アニーリング 制御された 焼鈍炉 (often a continuous electric furnace). This thermal treatment relieves internal stress and restores maximum ductility and electrical conductivity.
For multi-strand conductors (e.g., AAC, AAAC), single wires are gathered and twisted together using a Stranding Machine. This process increases the conductor’s flexibility, strength, and overall current-carrying capacity while maintaining the geometric precision of the final cable.
The final wire or cable is spooled onto reels, coils, or bobbins using automated Spooling and Coiling Machines. The finished product is then secured with protective wrapping and strapping to prevent physical damage and ensure it is ready for customer delivery and installation.
Linsy Alu.はISO 9001、ISO 14001、SGS、OHSAS 1800の認証を取得し、お客様に最高の品質を保証しています。