{"id":10927,"date":"2026-11-21T04:46:12","date_gmt":"2026-11-21T04:46:12","guid":{"rendered":"https:\/\/premiumalu.com\/?p=10927"},"modified":"2026-11-21T04:46:12","modified_gmt":"2026-11-21T04:46:12","slug":"7075-t7451-vs-t7351-plate-temper","status":"publish","type":"post","link":"https:\/\/premiumalu.com\/pt\/7075-t7451-vs-t7351-plate-temper\/","title":{"rendered":"7075 T7451 vs T7351: Escolher um ponto na escala de sobreenvelhecimento"},"content":{"rendered":"<h2 class=\"wp-block-heading\">O que \u00e9 o 7075-T7451?<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">O 7075-T7451 \u00e9 o t\u00eamper de chapa grossa do 7075 que se situa entre a resist\u00eancia m\u00e1xima e a m\u00e1xima resist\u00eancia \u00e0 corros\u00e3o. T7451 significa que a chapa foi submetida a tratamento t\u00e9rmico de solubiliza\u00e7\u00e3o, temperada em \u00e1gua, estirada 1,5\u20133% para remover tens\u00f5es residuais e, em seguida, sobreenvelhecida \u2014 mas n\u00e3o sobreenvelhecida tanto quanto o T7351. Esse meio-passo \u00e9 o objetivo central do t\u00eamper: mant\u00e9m mais resist\u00eancia que o T73, permanecendo muito mais resistente \u00e0 fissura\u00e7\u00e3o por corros\u00e3o sob tens\u00e3o que o T651.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\u00c9 um t\u00eamper de chapa, n\u00e3o de barra ou extrus\u00e3o. O estiramento \u00e9 o que torna a chapa grossa usin\u00e1vel e plana, e o sobreenvelhecimento \u00e9 o que impede que uma sec\u00e7\u00e3o espessa fissure sob tra\u00e7\u00e3o sustentada em servi\u00e7o h\u00famido ou com cloretos. Os equivalentes para barra e extrus\u00e3o t\u00eam as suas pr\u00f3prias designa\u00e7\u00f5es \u2014 T73511 para barra extrudida, por exemplo \u2014 e a numera\u00e7\u00e3o \u00e9 importante numa ordem de compra porque as propriedades variam com ela.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Quatro t\u00eamperes formam o conjunto a partir do qual est\u00e1 a escolher: T651, T7651, T7451 e T7351. N\u00e3o s\u00e3o quatro ligas diferentes nem quatro n\u00edveis de qualidade. S\u00e3o quatro pontos numa \u00fanica escala cont\u00ednua \u2014 at\u00e9 onde o tratamento de envelhecimento \u00e9 levado al\u00e9m do pico.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">Compreender a escala T7x<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">O 7075 no estado de pico de envelhecimento \u00e9 uma liga com um problema de corros\u00e3o. O T6 e a sua vers\u00e3o em chapa estirada T651 proporcionam a maior resist\u00eancia dispon\u00edvel em alum\u00ednio trabalhado e, num ambiente h\u00famido ou com cloretos, fissurar\u00e3o sob carga de tra\u00e7\u00e3o sustentada \u2014 um modo de falha que nenhum revestimento elimina. A resposta da ind\u00fastria foi o sobreenvelhecimento: envelhecer deliberadamente al\u00e9m do pico, aceitando menor resist\u00eancia em troca de uma microestrutura que resiste \u00e0 fissura\u00e7\u00e3o.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Cada um dos quatro t\u00eamperes \u00e9 uma resposta diferente a \"at\u00e9 onde al\u00e9m do pico\". O sufixo \"51\" \u00e9 constante em todos eles: significa que a chapa foi estirada ap\u00f3s a tempera, o que a chapa grossa necessita para estabilidade na maquinagem.<\/p>\n\n\n\n<h3 class=\"wp-block-heading\">T651 \u2014 Resist\u00eancia m\u00e1xima, sem sobreenvelhecimento<\/h3>\n\n\n\n<p class=\"wp-block-paragraph\">A refer\u00eancia de base. Maior resist\u00eancia dos quatro, pior resist\u00eancia \u00e0 fissura\u00e7\u00e3o por corros\u00e3o sob tens\u00e3o. Correto quando o ambiente de servi\u00e7o \u00e9 seco, protegido, ou a pe\u00e7a nunca est\u00e1 sujeita a tens\u00e3o de tra\u00e7\u00e3o sustentada na dire\u00e7\u00e3o transversal curta. \u00c9 o t\u00eamper em que a maior parte da chapa 7075 de stock \u00e9 fornecida, e aquele para o qual a maioria dos trabalhos gerais de maquinagem \u00e9 especificada.<\/p>\n\n\n\n<h3 class=\"wp-block-heading\">T7651 \u2014 Ligeiro sobreenvelhecimento, orientado para a esfolia\u00e7\u00e3o<\/h3>\n\n\n\n<p class=\"wp-block-paragraph\">O T7651 abdica de cerca de 3,5% da resist\u00eancia \u00e0 tra\u00e7\u00e3o do T651. O seu prop\u00f3sito \u00e9 mais restrito que os outros dois pontos de sobreenvelhecimento: visa a <strong>corros\u00e3o por esfolia\u00e7\u00e3o<\/strong>, a delamina\u00e7\u00e3o camada a camada que ataca as bordas da chapa e as superf\u00edcies maquinadas, em vez da fissura\u00e7\u00e3o por corros\u00e3o sob tens\u00e3o na dire\u00e7\u00e3o transversal curta. Uma chapa T7651 \u00e9 materialmente melhor que o T651 numa condi\u00e7\u00e3o de bordo exposto, e apenas modestamente melhor em SCC.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Vale a pena reter essa distin\u00e7\u00e3o, porque quebra a narrativa arrumada. O T76 e o T73 respondem a dois modos de falha diferentes, pelo que se devem ordenar estes t\u00eamperes pelo que protegem \u2014 n\u00e3o por qu\u00e3o sobreenvelhecidos est\u00e3o.<\/p>\n\n\n\n<h3 class=\"wp-block-heading\">T7451 \u2014 O ponto interm\u00e9dio<\/h3>\n\n\n\n<p class=\"wp-block-paragraph\">O T7451 \u00e9 um sobreenvelhecimento mais completo que o T7651, mas mais ligeiro que o T7351, e \u00e9 o t\u00eamper em torno do qual este artigo \u00e9 constru\u00eddo. Abdica de cerca de 8% da resist\u00eancia \u00e0 tra\u00e7\u00e3o do T651 e, em troca, proporciona resist\u00eancia \u00e0 SCC pr\u00f3xima da do T73 \u2014 ou seja, numa classe diferente do T651.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">A forma de o ter em mente: <strong>O T7451 \u00e9 um T7351 que n\u00e3o foi sobreenvelhecido tanto.<\/strong> Obt\u00e9m-se aproximadamente 6% mais resist\u00eancia \u00e0 tra\u00e7\u00e3o que o T7351 e abdica-se de uma parte da sua margem de corros\u00e3o. Para uma sec\u00e7\u00e3o espessa que tem de suportar carga real num ambiente h\u00famido, \u00e9 frequentemente a melhor troca.<\/p>\n\n\n\n<h3 class=\"wp-block-heading\">T7351 \u2014 Sobreenvelhecimento total<\/h3>\n\n\n\n<p class=\"wp-block-paragraph\">O mais sobreenvelhecido dos quatro. Cerca de 13% abaixo do T651 em resist\u00eancia \u00e0 tra\u00e7\u00e3o, e o mais resistente \u00e0 fissura\u00e7\u00e3o por corros\u00e3o sob tens\u00e3o \u2014 raz\u00e3o pela qual \u00e9 o padr\u00e3o para estrutura aeron\u00e1utica espessa na dire\u00e7\u00e3o transversal curta: nervuras de asa, refor\u00e7os de longarina, cavernas, anteparas e hardware de defesa onde uma fissura n\u00e3o \u00e9 um resultado aceit\u00e1vel a nenhum n\u00edvel de resist\u00eancia.<\/p>\n\n\n\n<figure class=\"wp-block-image size-large\"><img fetchpriority=\"high\" decoding=\"async\" width=\"1200\" height=\"896\" src=\"https:\/\/premiumalu.com\/wp-content\/uploads\/2026\/11\/02-overage-ladder.webp\" alt=\"Quatro provetes de chapa de alum\u00ednio 7075 maquinados com precis\u00e3o, dispostos lado a lado, ilustrando a escala de sobreenvelhecimento do T651 ao T7351\" class=\"wp-image-10925\" srcset=\"https:\/\/premiumalu.com\/wp-content\/uploads\/2026\/11\/02-overage-ladder.webp 1200w, https:\/\/premiumalu.com\/wp-content\/uploads\/2026\/11\/02-overage-ladder-300x224.webp 300w, https:\/\/premiumalu.com\/wp-content\/uploads\/2026\/11\/02-overage-ladder-1024x765.webp 1024w, https:\/\/premiumalu.com\/wp-content\/uploads\/2026\/11\/02-overage-ladder-768x573.webp 768w, https:\/\/premiumalu.com\/wp-content\/uploads\/2026\/11\/02-overage-ladder-16x12.webp 16w, https:\/\/premiumalu.com\/wp-content\/uploads\/2026\/11\/02-overage-ladder-600x448.webp 600w\" sizes=\"(max-width: 1200px) 100vw, 1200px\" \/><figcaption class=\"wp-element-caption\">A escala de sobreenvelhecimento da chapa 7075: avan\u00e7ar al\u00e9m da resist\u00eancia m\u00e1xima troca resist\u00eancia \u00e0 tra\u00e7\u00e3o por resist\u00eancia \u00e0 corros\u00e3o sob tens\u00e3o e \u00e0 esfolia\u00e7\u00e3o.<\/figcaption><\/figure>\n\n\n\n<h2 class=\"wp-block-heading\">Propriedades mec\u00e2nicas do 7075-T7451<\/h2>\n\n\n\n<figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><thead><tr><th>Temperamento<\/th><th>Tra\u00e7\u00e3o<\/th><th>Ced\u00eancia<\/th><th>Alongamento<\/th><th>vs T651 (tra\u00e7\u00e3o)<\/th><\/tr><\/thead><tbody><tr><td>T651<\/td><td>572 MPa<\/td><td>503 MPa<\/td><td>11%<\/td><td>refer\u00eancia de base<\/td><\/tr><tr><td>T7651<\/td><td>552 MPa<\/td><td>490 MPa<\/td><td>11%<\/td><td>\u22123,5%<\/td><\/tr><tr><td>T7451<\/td><td>524 MPa<\/td><td>469 MPa<\/td><td>11%<\/td><td>\u22128,4%<\/td><\/tr><tr><td>T7351<\/td><td>496 MPa<\/td><td>434 MPa<\/td><td>12%<\/td><td>\u221213,3%<\/td><\/tr><\/tbody><\/table><\/figure>\n\n\n\n<p class=\"wp-block-paragraph\">Valores t\u00edpicos de chapa segundo a ASTM B209 e as especifica\u00e7\u00f5es AMS de chapa correspondentes (AMS 4078 para T7351); o intervalo de aceita\u00e7\u00e3o para cada t\u00eamper e espessura \u00e9 definido por essa especifica\u00e7\u00e3o. Sec\u00e7\u00f5es mais espessas apresentam valores ligeiramente inferiores porque a taxa de tempera diminui com a espessura \u2014 retire os valores do certificado para a espessura que est\u00e1 a comprar.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Leia a coluna de percentagens, n\u00e3o a absoluta. No papel, 524 MPa contra 572 parece uma perda real. Em termos de projeto, a quest\u00e3o \u00e9 se precisa dos 8% superiores do intervalo de resist\u00eancia \u2014 e se a pe\u00e7a vive em humidade, sal ou cloretos, a resposta \u00e9 geralmente que n\u00e3o, porque os 8% extra do T651 v\u00eam com um modo de fissura\u00e7\u00e3o que n\u00e3o se anuncia.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Para um especificador: o T7451 mant\u00e9m aproximadamente 91% da resist\u00eancia \u00e0 tra\u00e7\u00e3o do T651 e a maior parte da resist\u00eancia \u00e0 SCC do T7351. \u00c9 uma posi\u00e7\u00e3o invulgarmente boa na curva, raz\u00e3o pela qual existe como t\u00eamper separado em vez de ser integrado num dos seus vizinhos.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">Onde cada ponto \u00e9 utilizado<\/h2>\n\n\n\n<h3 class=\"wp-block-heading\">T7451 \u2014 Estrutura portante em servi\u00e7o h\u00famido<\/h3>\n\n\n\n<p class=\"wp-block-paragraph\">Grandes componentes estruturais maquinados, acess\u00f3rios aeron\u00e1uticos que est\u00e3o sujeitos simultaneamente a carga e humidade, ferramentas e dispositivos de fixa\u00e7\u00e3o armazenados por longos per\u00edodos onde a estabilidade dimensional ao longo dos anos \u00e9 t\u00e3o importante quanto a resist\u00eancia. O fio condutor \u00e9 uma pe\u00e7a que tem de suportar uma carga calculada e n\u00e3o se pode contar que permane\u00e7a seca durante toda a sua vida \u00fatil.<\/p>\n\n\n\n<h3 class=\"wp-block-heading\">T7351 \u2014 Sec\u00e7\u00f5es espessas onde a fissura\u00e7\u00e3o \u00e9 inaceit\u00e1vel<\/h3>\n\n\n\n<p class=\"wp-block-paragraph\">Nervuras de asa, refor\u00e7os e almas de longarina, cavernas, anteparas, estrutura pesada de defesa. S\u00e3o sec\u00e7\u00f5es espessas carregadas na dire\u00e7\u00e3o transversal curta, que \u00e9 exatamente onde o 7075 no pico de envelhecimento \u00e9 mais fraco contra a SCC. O sacrif\u00edcio de 13% de resist\u00eancia \u00e9 o pre\u00e7o de n\u00e3o ter uma fissura a iniciar-se numa pe\u00e7a que ningu\u00e9m consegue inspecionar por dentro.<\/p>\n\n\n\n<h3 class=\"wp-block-heading\">T7651 e T651 \u2014 Bordas expostas e servi\u00e7o seco<\/h3>\n\n\n\n<p class=\"wp-block-paragraph\">T7651 para chapa cujas bordas e superf\u00edcies maquinadas estar\u00e3o expostas \u00e0s intemp\u00e9ries e onde a esfolia\u00e7\u00e3o \u00e9 a preocupa\u00e7\u00e3o. T651 para pe\u00e7as secas, protegidas e cr\u00edticas em resist\u00eancia \u2014 o trabalho geral de maquinagem, moldes e automa\u00e7\u00e3o em que a maior parte da chapa 7075 realmente \u00e9 aplicada.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">T7451 vs T7351 vs T7651 vs T651 \u2014 Como escolher<\/h2>\n\n\n\n<figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><thead><tr><th>Propriedade<\/th><th>T651<\/th><th>T7651<\/th><th>T7451<\/th><th>T7351<\/th><\/tr><\/thead><tbody><tr><td>Tra\u00e7\u00e3o<\/td><td>572 MPa<\/td><td>552 MPa<\/td><td>524 MPa<\/td><td>496 MPa<\/td><\/tr><tr><td>Resist\u00eancia \u00e0 SCC<\/td><td>Ruim<\/td><td>Moderado<\/td><td>Bom, pr\u00f3ximo do T73<\/td><td>Melhor<\/td><\/tr><tr><td>Resist\u00eancia \u00e0 esfolia\u00e7\u00e3o<\/td><td>Ruim<\/td><td>Bom<\/td><td>Bom<\/td><td>Bom<\/td><\/tr><tr><td>Estabilidade de usinagem<\/td><td>Bom (estirado)<\/td><td>Bom<\/td><td>Bom<\/td><td>Bom<\/td><\/tr><tr><td>Melhor para<\/td><td>Seco, protegido, resist\u00eancia m\u00e1xima<\/td><td>Bordas expostas, risco de esfolia\u00e7\u00e3o<\/td><td>Carga mais humidade<\/td><td>Sec\u00e7\u00f5es espessas, cr\u00edticas quanto a fissura\u00e7\u00e3o<\/td><\/tr><\/tbody><\/table><\/figure>\n\n\n\n<figure class=\"wp-block-image size-large\"><img decoding=\"async\" width=\"1200\" height=\"896\" src=\"https:\/\/premiumalu.com\/wp-content\/uploads\/2026\/11\/03-st-cracking-risk.webp\" alt=\"Compara\u00e7\u00e3o macro de dois blocos espessos de alum\u00ednio 7075 sob carregamento de tra\u00e7\u00e3o transversal curto, mostrando microfissura\u00e7\u00e3o no T651 versus imunidade \u00e0 fissura\u00e7\u00e3o no T7451\" class=\"wp-image-10926\" srcset=\"https:\/\/premiumalu.com\/wp-content\/uploads\/2026\/11\/03-st-cracking-risk.webp 1200w, https:\/\/premiumalu.com\/wp-content\/uploads\/2026\/11\/03-st-cracking-risk-300x224.webp 300w, https:\/\/premiumalu.com\/wp-content\/uploads\/2026\/11\/03-st-cracking-risk-1024x765.webp 1024w, https:\/\/premiumalu.com\/wp-content\/uploads\/2026\/11\/03-st-cracking-risk-768x573.webp 768w, https:\/\/premiumalu.com\/wp-content\/uploads\/2026\/11\/03-st-cracking-risk-16x12.webp 16w, https:\/\/premiumalu.com\/wp-content\/uploads\/2026\/11\/03-st-cracking-risk-600x448.webp 600w\" sizes=\"(max-width: 1200px) 100vw, 1200px\" \/><figcaption class=\"wp-element-caption\">Carregamento de tra\u00e7\u00e3o na dire\u00e7\u00e3o transversal curta (ST) em chapa espessa: o T651 apresenta alto risco de fissura\u00e7\u00e3o por corros\u00e3o sob tens\u00e3o ao longo dos contornos de gr\u00e3o de lamina\u00e7\u00e3o; o T7451 e o T7351 proporcionam imunidade \u00e0 fissura\u00e7\u00e3o.<\/figcaption><\/figure>\n\n\n\n<p class=\"wp-block-paragraph\">Comece com duas perguntas, nesta ordem. <strong>Existe tens\u00e3o de tra\u00e7\u00e3o sustentada na dire\u00e7\u00e3o transversal curta?<\/strong> Se sim, o T651 est\u00e1 descartado \u2014 passe para o T7451 ou T7351. <strong>A sec\u00e7\u00e3o \u00e9 espessa o suficiente para que uma fissura n\u00e3o pudesse ser encontrada antes de se tornar cr\u00edtica?<\/strong> Se sim, T7351. Se a pe\u00e7a for usin\u00e1vel, suportar carga mas tiver sec\u00e7\u00e3o moderada, o T7451 \u00e9 geralmente a melhor escolha, e o T7651 s\u00f3 entra quando a esfolia\u00e7\u00e3o nas bordas expostas \u00e9 a preocupa\u00e7\u00e3o espec\u00edfica.<\/p>\n\n\n\n<h3 class=\"wp-block-heading\">Quando o T7451 \u00c9 a Escolha Certa<\/h3>\n\n\n\n<p class=\"wp-block-paragraph\">Duas condi\u00e7\u00f5es em conjunto: a pe\u00e7a suporta uma carga calculada e n\u00e3o \u00e9 poss\u00edvel garantir que permane\u00e7a seca durante a sua vida \u00fatil. Acess\u00f3rios aeron\u00e1uticos, estruturas pr\u00f3ximas de ambientes marinhos, ferramentas de longa dura\u00e7\u00e3o em instala\u00e7\u00f5es h\u00famidas. Nessas condi\u00e7\u00f5es, o sacrif\u00edcio de 8% de resist\u00eancia do T7451 compra uma margem de corros\u00e3o que o T651 n\u00e3o tem, a uma resist\u00eancia que o T7351 n\u00e3o consegue atingir.<\/p>\n\n\n\n<h3 class=\"wp-block-heading\">Quando o T7351 Se Adequa Melhor<\/h3>\n\n\n\n<p class=\"wp-block-paragraph\">Quando a sec\u00e7\u00e3o \u00e9 espessa e o modo de falha \u00e9 aquele que n\u00e3o se consegue inspecionar. Carregamento transversal curto em chapa pesada, estruturas de defesa, qualquer situa\u00e7\u00e3o em que uma fissura que se inicie no interior da pe\u00e7a seja pior do que 60 MPa de resist\u00eancia perdida. N\u00e3o use o T7451 aqui para poupar resist\u00eancia \u2014 a troca corre no sentido errado.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">Trabalhar com 7075-T7451 \u2014 Maquinagem, Corros\u00e3o, Acabamento<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>**Usinagem:**<\/strong> o estiramento no \"51\" \u00e9 o que faz isto funcionar. Uma chapa T7451 maquinada numa pe\u00e7a de parede fina mant\u00e9m-se plana onde uma chapa T6 se deformaria \u00e0 medida que o material \u00e9 removido. Corte-a com metal duro afiado e bom fluido de corte; o 7075 nesta dureza n\u00e3o \u00e9 tolerante a uma ferramenta que ro\u00e7a.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>Prote\u00e7\u00e3o contra corros\u00e3o:<\/strong> O T7451 resiste ao SCC muito melhor do que o T651, mas continua a ser uma liga 7xxx com cobre e com resist\u00eancia moderada \u00e0 corros\u00e3o geral. Anodize (Tipo II ou III) ou aplique um revestimento de convers\u00e3o nas superf\u00edcies expostas, e nunca confie no revenido sobreenvelhecido como substituto de um acabamento em servi\u00e7o com sais.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>Acabamento:<\/strong> a anodiza\u00e7\u00e3o \u00e9 rotineira, embora o 7075 receba um revestimento mais escuro e menos uniforme do que o 6xxx, e a anodiza\u00e7\u00e3o dura seja mais comum do que a anodiza\u00e7\u00e3o decorativa nesta liga. Mascare ou mandrile os furos cr\u00edticos ap\u00f3s o revestimento, uma vez que a camada de \u00f3xido altera as dimens\u00f5es.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>Soldagem:<\/strong> n\u00e3o \u00e9 uma liga para soldadura. O 7075, em qualquer tempera, geralmente n\u00e3o \u00e9 soldado por fus\u00e3o para servi\u00e7o estrutural; projete para fixa\u00e7\u00e3o mec\u00e2nica ou passe para uma liga sold\u00e1vel se a junta for estrutural.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">Vantagens e Limita\u00e7\u00f5es em Resumo<\/h2>\n\n\n\n<figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><thead><tr><th>Dimens\u00e3o<\/th><th>Vantagem<\/th><th>Quanto custa<\/th><\/tr><\/thead><tbody><tr><td>For\u00e7a<\/td><td>524 MPa de tra\u00e7\u00e3o \u2014 acima do T7351, pr\u00f3ximo do T651<\/td><td>8% abaixo do pico do T651<\/td><\/tr><tr><td>Resist\u00eancia \u00e0 SCC<\/td><td>Pr\u00f3ximo do T73, muito melhor do que o T651<\/td><td>N\u00e3o \u00e9 igual ao T7351 no pior caso transversal curto<\/td><\/tr><tr><td>Estabilidade de usinagem<\/td><td>O estiramento mant\u00e9m as pe\u00e7as de parede fina planas<\/td><td>Chapa espessa requer capacidade de estiramento, o que limita o fornecimento<\/td><\/tr><tr><td>Corros\u00e3o, geral<\/td><td>Melhor do que o T651 em servi\u00e7o h\u00famido<\/td><td>Continua a necessitar de revestimento em ambiente salino ou com cloretos<\/td><\/tr><tr><td>Esfolia\u00e7\u00e3o<\/td><td>Bom<\/td><td>O T7651 \u00e9 a tempera especificamente orientada para isto<\/td><\/tr><tr><td>Soldabilidade<\/td><td>\u2014<\/td><td>N\u00e3o \u00e9 uma liga de soldadura por fus\u00e3o em qualquer tempera<\/td><\/tr><\/tbody><\/table><\/figure>\n\n\n\n<h2 class=\"wp-block-heading\">Conclus\u00e3o<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">O 7075-T7451 n\u00e3o \u00e9 \"um T7351 mais resistente\" nem \"um T651 mais seguro\". \u00c9 um ponto deliberado num eixo: cerca de 8% abaixo da resist\u00eancia de pico, com a maior parte da resist\u00eancia \u00e0 corros\u00e3o sob tens\u00e3o que custa ao T7351 mais 5 pontos. Para chapa espessa que suporta carga e n\u00e3o pode ser mantida seca, essa \u00e9 geralmente a melhor troca dispon\u00edvel \u2014 e \u00e9 por isso que a tempera existe.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Fornecemos chapa 7075-T7451 e T7351, juntamente com T651 e T7651, com Certificado de Ensaio de F\u00e1brica em cada encomenda. A chapa espessa sobreenvelhecida depende da capacidade de estiramento, pelo que o prazo de entrega \u00e9 cotado em fun\u00e7\u00e3o da espessura e do tamanho necess\u00e1rios.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Envie-nos o desenho da pe\u00e7a com a tempera, espessura e ambiente de servi\u00e7o, e confirmaremos qual o patamar da escala que se adequa e cotaremos em conformidade.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">Perguntas frequentes<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>O T7451 \u00e9 mais resistente do que o T7351?<\/strong><\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Sim. Em chapa conforme a ASTM B209, o T7451 apresenta cerca de 524 MPa contra 496 para o T7351 \u2014 aproximadamente 6% mais em tra\u00e7\u00e3o e cerca de 8% mais em limite de ced\u00eancia \u2014 porque \u00e9 menos sobreenvelhecido. Perde alguma resist\u00eancia ao SCC por isso; ambos excedem largamente o T651.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>Posso usar T7451 em vez de T651?<\/strong><\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Apenas se o ambiente o justificar. O T7451 custa cerca de 8% da resist\u00eancia \u00e0 tra\u00e7\u00e3o do T651. Fa\u00e7a essa troca quando a pe\u00e7a estiver sujeita a tens\u00e3o de tra\u00e7\u00e3o sustentada em humidade ou cloretos, onde o T651 \u00e9 sens\u00edvel ao SCC.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>O que significa o \"51\" em T7451?<\/strong><\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Al\u00edvio de tens\u00f5es por estiramento, 1,5\u20133% ap\u00f3s a t\u00eampera. \u00c9 o que permite maquinar chapa espessa plana. Sem o estiramento, a tempera seria T74, que n\u00e3o \u00e9 um produto em chapa.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>Qual \u00e9 o pedido m\u00ednimo e o prazo de entrega?<\/strong><\/p>\n\n\n\n<p class=\"wp-block-paragraph\">MOQ baixo, tipicamente 10\u201360 dias dependendo da tempera, espessura e tamanho. A chapa espessa sobreenvelhecida depende da capacidade de estiramento, pelo que confirme a espessura antes de ser cotada uma data firme.<\/p>","protected":false},"excerpt":{"rendered":"<p>What Is 7075-T7451? 7075-T7451 is the 7075 thick-plate temper that sits between peak strength and maximum corrosion resistance. T7451 means the plate was solution heat treated, water quenched, stretched 1.5\u20133% to remove residual stress, then overaged \u2014 but not overaged as far as T7351. That half-step is the whole point of the temper: it keeps [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":10924,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_seopress_titles_title":"7075 T7451 vs T7351: Which Plate Temper?","_seopress_titles_desc":"7075-T7451 sits between T651 strength and T7351 corrosion resistance. Compare all four plate tempers, the strength each gives up, and which one to specify.","_seopress_robots_index":"","_seopress_robots_follow":"","_seopress_robots_imageindex":"","_seopress_robots_snippet":"","_seopress_robots_primary_cat":"","_seopress_robots_breadcrumbs":"","_seopress_robots_freeze_modified_date":"","_seopress_robots_custom_modified_date":"","_seopress_robots_canonical":"","_seopress_social_fb_title":"","_seopress_social_fb_desc":"","_seopress_social_fb_img":"","_seopress_social_fb_img_attachment_id":0,"_seopress_social_fb_img_width":0,"_seopress_social_fb_img_height":0,"_seopress_social_twitter_title":"","_seopress_social_twitter_desc":"","_seopress_social_twitter_img":"","_seopress_social_twitter_img_attachment_id":0,"_seopress_social_twitter_img_width":0,"_seopress_social_twitter_img_height":0,"_seopress_redirections_value":"","_seopress_redirections_enabled":"","_seopress_redirections_enabled_regex":"","_seopress_redirections_logged_status":"","_seopress_redirections_param":"","_seopress_redirections_type":0,"_seopress_analysis_target_kw":"","footnotes":""},"categories":[179,180],"tags":[],"class_list":["post-10927","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-7000-series-aluminum","category-aluminum-alloy"],"_links":{"self":[{"href":"https:\/\/premiumalu.com\/pt\/wp-json\/wp\/v2\/posts\/10927","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/premiumalu.com\/pt\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/premiumalu.com\/pt\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/premiumalu.com\/pt\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/premiumalu.com\/pt\/wp-json\/wp\/v2\/comments?post=10927"}],"version-history":[{"count":1,"href":"https:\/\/premiumalu.com\/pt\/wp-json\/wp\/v2\/posts\/10927\/revisions"}],"predecessor-version":[{"id":10940,"href":"https:\/\/premiumalu.com\/pt\/wp-json\/wp\/v2\/posts\/10927\/revisions\/10940"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/premiumalu.com\/pt\/wp-json\/wp\/v2\/media\/10924"}],"wp:attachment":[{"href":"https:\/\/premiumalu.com\/pt\/wp-json\/wp\/v2\/media?parent=10927"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/premiumalu.com\/pt\/wp-json\/wp\/v2\/categories?post=10927"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/premiumalu.com\/pt\/wp-json\/wp\/v2\/tags?post=10927"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}