{"id":8323,"date":"2025-03-23T12:22:41","date_gmt":"2025-03-23T12:22:41","guid":{"rendered":"https:\/\/premiumalu.com\/master-6106-aluminum-techniques-expert-tips\/"},"modified":"2026-10-06T14:51:03","modified_gmt":"2026-10-06T14:51:03","slug":"master-6106-alumi%cc%87nyum-tekni%cc%87kleri%cc%87-uzman-i%cc%87puclari","status":"publish","type":"post","link":"https:\/\/premiumalu.com\/tr\/master-6106-aluminum-techniques-expert-tips\/","title":{"rendered":"Master 6106 Al\u00fcminyum Teknikleri: Uzman Rehberi"},"content":{"rendered":"<p class=\"wp-block-paragraph\">6106, orta mukavemetli, \u0131s\u0131l i\u015flemle sertle\u015ftirilebilen bir 6xxx ekstr\u00fczyon ala\u015f\u0131m\u0131d\u0131r. Tan\u0131mlay\u0131c\u0131 \u00f6zelli\u011fi ekstr\u00fcde edilebilirli\u011fidir: daha g\u00fc\u00e7l\u00fc 6xxx kalitelerinin dolduramayaca\u011f\u0131 ince, karma\u015f\u0131k kesitlere akar. 6061'den daha az magnezyum ve silisyum i\u00e7erir ve bu daha yal\u0131n kimya as\u0131l meseledir \u2014 6061 veya 6082'nin ba\u015farabildi\u011finden daha ince cidarlara ve daha karma\u015f\u0131k kesitlere ekstr\u00fcde edilebilir, bunu yaparken de <a href=\"https:\/\/premiumalu.com\/tr\/6063-aluminyum-ekstruzyonlar-icin-uzman-ipuclari\/\">6063<\/a> mukavemet a\u00e7\u0131s\u0131ndan daha y\u00fcksek performans g\u00f6sterir. Tipik kullan\u0131mlar\u0131 yap\u0131sald\u0131r: merdivenler ve eri\u015fim kuleleri, demiryolu ta\u015f\u0131tlar\u0131, otomotiv yap\u0131lar\u0131 ve g\u00fcverte \u00fcst\u00fc deniz yap\u0131lar\u0131.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">\u0130lk kez spesifikasyon yapanlar\u0131 iki \u015fey yan\u0131lt\u0131r. Birincisi formdur: 6106 haddelenmi\u015f bir tan\u0131m de\u011fildir, dolay\u0131s\u0131yla ASTM B209'a g\u00f6re 6106 plaka veya sac belirten bir \u00e7izimin arkas\u0131nda standart bir \u00fcr\u00fcn yoktur. \u0130kincisi kaynakt\u0131r. 6106 mukavemetini so\u011fuk \u015fekillendirmeden de\u011fil \u0131s\u0131l i\u015flemden ald\u0131\u011f\u0131 i\u00e7in, bir ark kayna\u011f\u0131 mukavemetin b\u00fcy\u00fck bir k\u0131sm\u0131n\u0131 yerel olarak ortadan kald\u0131r\u0131r ve bu kay\u0131p birle\u015fimin nas\u0131l boyutland\u0131r\u0131laca\u011f\u0131n\u0131 belirler.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">6106 Al\u00fcminyum Nedir?<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">6106, 6000 serisinde yer alan bir al\u00fcminyum\u2013magnezyum\u2013silisyum ala\u015f\u0131m\u0131d\u0131r (manganez ile birlikte) ve ilk olarak 1979'da tescil edilmi\u015ftir. \u00c7izimlerde ve fabrika belgelerinde g\u00f6rece\u011finiz tan\u0131mlar:<\/p>\n\n\n\n<figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td>Tan\u0131mlama sistemi<\/td><td>De\u011fer<\/td><\/tr><tr><td>Al\u00fcminyum Derne\u011fi (AA)<\/td><td>6106<\/td><\/tr><tr><td>UNS<\/td><td>A96106<\/td><\/tr><tr><td>EN say\u0131sal \/ kimyasal<\/td><td>EN AW-6106 \/ AlMgSiMn<\/td><\/tr><tr><td>\u00c7in standard\u0131<\/td><td>GB\/T 3190<\/td><\/tr><tr><td>Analitik kontrol i\u00e7in bile\u015fim s\u0131n\u0131rlar\u0131<\/td><td>EN 573-3<\/td><\/tr><tr><td>Ekstr\u00fcde \u00fcr\u00fcn mekanik de\u011ferleri<\/td><td>EN 755-2<\/td><\/tr><tr><td>Ekstr\u00fcde \u00e7ubuk, \u00e7ubuk, tel, profil, boru<\/td><td>ASTM B221<\/td><\/tr><tr><td>Ekstr\u00fcde \u00e7ubuk, bar, boru, profil (ISO)<\/td><td>ISO 6362-2<\/td><\/tr><\/tbody><\/table><\/figure>\n\n\n\n<p class=\"wp-block-paragraph\">\u00c7o\u011fu Avrupal\u0131 stok\u00e7unun kulland\u0131\u011f\u0131 ala\u015f\u0131m tan\u0131m\u0131, tasar\u0131m amac\u0131n\u0131 bir veri sayfas\u0131ndan daha iyi \u00f6zetler: 6000 serisiyle ili\u015fkili korozyon direncini, kaynaklanabilirli\u011fi ve \u015fekillendirilebilirli\u011fi korurken, mekanik \u00f6zellikler, \u015fekil karma\u015f\u0131kl\u0131\u011f\u0131, minimum kesit kal\u0131nl\u0131\u011f\u0131 ve y\u00fczey kalitesinin mevcut en iyi kombinasyonunu sunmay\u0131 ama\u00e7layan bir ekstr\u00fczyon ala\u015f\u0131m\u0131. 6082 gibi daha g\u00fc\u00e7l\u00fc ala\u015f\u0131mlarda \u00fcretilemeyen kesitler rutin olarak 6106'da \u00fcretilir.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Bu konum, herhangi bir tek \u00f6zellik de\u011ferinden daha \u00f6nemlidir. 6xxx ala\u015f\u0131mlar\u0131n\u0131 6063'ten 6106 \u00fczerinden 6061 ve 6082'ye uzanan bir eksende d\u00fc\u015f\u00fcn\u00fcrseniz, sa\u011fa do\u011fru ilerledik\u00e7e ekstr\u00fcde edilebilirlik d\u00fc\u015fer ve mukavemet artar. 6106 kas\u0131tl\u0131 olarak ortada yer al\u0131r ve o \u00e7izginin hi\u00e7bir ucunun i\u015fe yaramad\u0131\u011f\u0131 durumlarda yerini hak eder.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">Kimyasal Bile\u015fim<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">A\u015fa\u011f\u0131daki s\u0131n\u0131rlar EN 573-3 ve Aluminum Association tescilini takip eder. Her \u015fey a\u011f\u0131rl\u0131k y\u00fczdesi cinsindendir, geri kalan al\u00fcminyumdur.<\/p>\n\n\n\n<figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td>Element<\/td><td>Kompozisyon (%)<\/td><\/tr><tr><td>Silisyum (Si)<\/td><td>0.30 \u2013 0.60<\/td><\/tr><tr><td>Magnezyum (Mg)<\/td><td>0.40 \u2013 0.80<\/td><\/tr><tr><td>Manganez (Mn)<\/td><td>0.05 - 0.20<\/td><\/tr><tr><td>Demir (Fe)<\/td><td>0,35 maks.<\/td><\/tr><tr><td>Bak\u0131r (Cu)<\/td><td>0,25 maks.<\/td><\/tr><tr><td>Krom (Cr)<\/td><td>0,20 maks.<\/td><\/tr><tr><td>\u00c7inko (Zn)<\/td><td>0,10 maks.<\/td><\/tr><tr><td>Titanyum (Ti)<\/td><td>0,10 maks.<\/td><\/tr><tr><td>Di\u011ferleri, her biri<\/td><td>0,05 maks.<\/td><\/tr><tr><td>Di\u011ferleri, toplam<\/td><td>0,15 maks.<\/td><\/tr><\/tbody><\/table><\/figure>\n\n\n\n<p class=\"wp-block-paragraph\">Bunu 6061 ile kar\u015f\u0131la\u015ft\u0131rarak okuyun; 6061 yakla\u015f\u0131k 0,8\u20131,2% magnezyum, 0,4\u20130,8% silisyum i\u00e7erir ve 0,15\u20130,4% bak\u0131r ekler. Bu fark, iki ala\u015f\u0131m aras\u0131ndaki neredeyse t\u00fcm davran\u0131\u015f fark\u0131n\u0131 a\u00e7\u0131klar:<\/p>\n\n\n\n<ul class=\"wp-block-list\">\n<li><strong>Daha d\u00fc\u015f\u00fck Mg + Si toplam\u0131<\/strong> g\u00fc\u00e7lendirme i\u00e7in mevcut daha az Mg\u2082Si \u00e7\u00f6keltisi anlam\u0131na gelir, dolay\u0131s\u0131yla tepe mukavemet daha d\u00fc\u015f\u00fckt\u00fcr \u2014 ancak al\u00fcminyumda \u00e7\u00f6z\u00fcnm\u00fc\u015f halde kalan ala\u015f\u0131m elementi de daha azd\u0131r, bu nedenle elektriksel iletkenlik daha y\u00fcksektir ve ekstr\u00fczyon s\u0131ras\u0131ndaki ak\u0131\u015f gerilmesi daha d\u00fc\u015f\u00fckt\u00fcr.<\/li>\n\n\n\n<li><strong>\u00c7ok d\u00fc\u015f\u00fck bak\u0131r<\/strong> korozyon davran\u0131\u015f\u0131n\u0131 temiz tutar ve anodizasyon tutarl\u0131l\u0131\u011f\u0131na yard\u0131mc\u0131 olur. Ayr\u0131ca 6106'n\u0131n bak\u0131r i\u00e7eren 6xxx ala\u015f\u0131mlar\u0131n\u0131n pe\u015finden gidebilece\u011fi \u015fekilde mukavemet pe\u015finde ko\u015famayaca\u011f\u0131 anlam\u0131na gelir.<\/li>\n\n\n\n<li><strong>Manganez kas\u0131tl\u0131 olarak mevcuttur<\/strong> (0,05\u20130,20%), \u00e7o\u011fu 6xxx kalitesinin aksine burada yaln\u0131zca bir safs\u0131zl\u0131k de\u011fildir. Mn, yeniden kristalle\u015fme yoluyla tane yap\u0131s\u0131n\u0131 kontrol eder ve ekstr\u00fcde kesitin toklu\u011funu ve y\u00fczey kalitesini iyile\u015ftirir.<\/li>\n\n\n\n<li><strong>S\u0131k\u0131 demir kontrol\u00fc<\/strong> anodizasyon i\u00e7in \u00f6nemlidir. Demir i\u00e7eren intermetalikler, \u015feffaf anodize kaplamada \u00e7izgiler ve gri benekler olarak ortaya \u00e7\u0131kan \u015feylerdir.<\/li>\n<\/ul>\n\n\n\n<h2 class=\"wp-block-heading\">Temperlere G\u00f6re Mekanik \u00d6zellikler<\/h2>\n\n\n\n<figure class=\"wp-block-image size-full\"><img fetchpriority=\"high\" decoding=\"async\" width=\"800\" height=\"600\" src=\"https:\/\/premiumalu.com\/wp-content\/uploads\/2025\/03\/Mechanical-Properties-by-Temper-2.png\" alt=\"\" class=\"wp-image-10651\" srcset=\"https:\/\/premiumalu.com\/wp-content\/uploads\/2025\/03\/Mechanical-Properties-by-Temper-2.png 800w, https:\/\/premiumalu.com\/wp-content\/uploads\/2025\/03\/Mechanical-Properties-by-Temper-2-300x225.png 300w, https:\/\/premiumalu.com\/wp-content\/uploads\/2025\/03\/Mechanical-Properties-by-Temper-2-768x576.png 768w, https:\/\/premiumalu.com\/wp-content\/uploads\/2025\/03\/Mechanical-Properties-by-Temper-2-16x12.png 16w, https:\/\/premiumalu.com\/wp-content\/uploads\/2025\/03\/Mechanical-Properties-by-Temper-2-600x450.png 600w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/><\/figure>\n\n\n\n<p class=\"wp-block-paragraph\">6106 mukavemetini \u00e7\u00f6zeltiye alma \u0131s\u0131l i\u015flemi ve ard\u0131ndan ya\u015fland\u0131rma ile kazan\u0131r, bu nedenle sat\u0131r kalemindeki temper, par\u00e7an\u0131n nas\u0131l davranaca\u011f\u0131na dair neredeyse her \u015feyi belirler. A\u015fa\u011f\u0131daki de\u011ferler <strong>tipiktir<\/strong>; kabul\u00fc fiilen y\u00f6neten say\u0131lar \u00fcr\u00fcn standard\u0131ndaki minimumlard\u0131r ve bunlar sipari\u015f edilen spesifik profil ve cidar kal\u0131nl\u0131\u011f\u0131 i\u00e7in fabrika muayene sertifikas\u0131na g\u00f6re do\u011frulanmal\u0131d\u0131r.<\/p>\n\n\n\n<figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td>Temper<\/td><td>Tipik \u00e7ekme mukavemeti (MPa)<\/td><td>Tipik akma mukavemeti (MPa)<\/td><td>Tipik uzama (1%)<\/td><td>Tipik kullan\u0131m<\/td><\/tr><tr><td>O (tavlanm\u0131\u015f)<\/td><td>~110<\/td><td>~60<\/td><td>~22<\/td><td>Daha ileri i\u015flem \u00f6ncesi \u015fekillendirme sto\u011fu<\/td><\/tr><tr><td>T4 (\u00e7\u00f6zeltiye al\u0131nm\u0131\u015f, do\u011fal ya\u015fland\u0131r\u0131lm\u0131\u015f)<\/td><td>~200<\/td><td>~120<\/td><td>~16<\/td><td>B\u00fck\u00fcn veya \u015fekillendirin, ard\u0131ndan T6'ya ya\u015fland\u0131r\u0131n<\/td><\/tr><tr><td>T5 (presle su verilmi\u015f, yapay ya\u015fland\u0131r\u0131lm\u0131\u015f)<\/td><td>~220<\/td><td>~165<\/td><td>~12<\/td><td>Maliyet hassasiyetli yap\u0131sal ekstr\u00fczyonlar<\/td><\/tr><tr><td>T6 (\u00e7\u00f6zeltiye al\u0131nm\u0131\u015f, yapay ya\u015fland\u0131r\u0131lm\u0131\u015f)<\/td><td>~290<\/td><td>~220<\/td><td>9 \u2013 14<\/td><td>Standart yap\u0131sal spesifikasyon<\/td><\/tr><\/tbody><\/table><\/figure>\n\n\n\n<p class=\"wp-block-paragraph\">10 mm cidar kal\u0131nl\u0131\u011f\u0131na kadar profiller i\u00e7in EN 755-2, T6 durumunda minimum de\u011ferleri \u015f\u00f6yle belirler: <strong>250 MPa \u00e7ekme, 200 MPa akma gerilmesi ve 6% uzama<\/strong>. Bu minimumlar\u0131n tipik rakamlardan ne kadar d\u00fc\u015f\u00fck oldu\u011funa dikkat edin: bu fark normaldir, cidar kal\u0131nl\u0131\u011f\u0131yla geni\u015fler ve bu nedenle tasar\u0131m ya standart minimumu ya da MTC de\u011ferini kullanmal\u0131d\u0131r \u2014 asla bir veri sayfas\u0131ndan al\u0131nt\u0131lanan tipik bir rakam\u0131 de\u011fil.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Tablodan \u00fc\u00e7 pratik sonu\u00e7 \u00e7\u0131kar:<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>T5, T6'dan \u00f6nce fiyatland\u0131rmaya de\u011ferdir.<\/strong> T5 su verme i\u015flemini ayr\u0131 bir f\u0131r\u0131n \u00e7evrimi yerine ekstr\u00fczyon presinden al\u0131r, bu da bir proses ad\u0131m\u0131n\u0131 ortadan kald\u0131r\u0131r ve genellikle maliyeti d\u00fc\u015f\u00fcr\u00fcr. Bir\u00e7ok yap\u0131sal kesit i\u00e7in mukavemet fark\u0131 tasar\u0131m\u0131 de\u011fi\u015ftirmez, dolay\u0131s\u0131yla T6 al\u0131\u015fkanl\u0131k gere\u011fi belirtildi\u011finde masada kalan ger\u00e7ek parad\u0131r.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>\u015eekillendirme nihai ya\u015fland\u0131rmadan \u00f6nce yap\u0131lmal\u0131d\u0131r.<\/strong> T6\u201cda so\u011fuk \u015fekillendirme m\u00fcmk\u00fcnd\u00fcr ancak s\u0131n\u0131rl\u0131d\u0131r. T6\u201dda \u00e7atlayacak b\u00fck\u00fcmler O veya T4\u201cte sorunsuzdur ve par\u00e7a daha sonra T6 \u00f6zelliklerine ula\u015fmak i\u00e7in ya\u015fland\u0131r\u0131labilir. Mevcut s\u0131ralaman\u0131z \u201dT6 ekstr\u00fcde et, sonra b\u00fck\" ise, bunun yerine \"T4 \u015fekillendir, sonra ya\u015fland\u0131r\"\u0131n i\u015fe yaray\u0131p yaramad\u0131\u011f\u0131n\u0131 sorun.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>Kal\u0131nl\u0131k cevab\u0131 de\u011fi\u015ftirir.<\/strong> Yay\u0131mlanan minimumlar bir nedenden dolay\u0131 cidar kal\u0131nl\u0131\u011f\u0131na ba\u011fl\u0131d\u0131r: daha kal\u0131n kesitler daha yava\u015f so\u011fur, bu nedenle daha az ala\u015f\u0131m elementi \u00e7\u00f6zeltide kal\u0131r ve daha sonra daha az g\u00fc\u00e7lendirici \u00e7\u00f6kelti olu\u015fur. Kal\u0131n cidarl\u0131 bir 6106 profili, ince cidarl\u0131 bir profilin ula\u015ft\u0131\u011f\u0131 de\u011ferlere ula\u015fmaz ve ger\u00e7ek kesit i\u00e7in MTC tek g\u00fcvenilir kay\u0131tt\u0131r.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">Fiziksel \u00d6zellikler<\/h2>\n\n\n\n<figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td>M\u00fclkiyet<\/td><td>De\u011fer<\/td><\/tr><tr><td>Yo\u011funluk<\/td><td>2,70 g\/cm\u00b3<\/td><\/tr><tr><td>Erime aral\u0131\u011f\u0131 (solidus\u2013liquidus)<\/td><td>~610 \u2013 660 \u00b0C<\/td><\/tr><tr><td>Elastisite mod\u00fcl\u00fc<\/td><td>~69.5 GPa<\/td><\/tr><tr><td>Termal genle\u015fme katsay\u0131s\u0131<\/td><td>~23.4 \u00d7 10\u207b\u2076 \/K<\/td><\/tr><tr><td>Termal iletkenlik<\/td><td>~190 W\/m\u00b7K<\/td><\/tr><tr><td>Electrical conductivity (equal volume)<\/td><td>~49 % IACS<\/td><\/tr><tr><td>Maximum continuous service temperature<\/td><td>~160 \u00b0C<\/td><\/tr><tr><td>Fatigue strength (T6)<\/td><td>~88 MPa<\/td><\/tr><\/tbody><\/table><\/figure>\n\n\n\n<p class=\"wp-block-paragraph\">Two of these deserve a note because they are routinely misread.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>Thermal expansion does not separate 6106 from 6061.<\/strong> 6106 measures about 23.4 \u00d7 10\u207b\u2076\/K and 6061 about 23.6 \u00d7 10\u207b\u2076\/K. Any comparison table you see listing &#8220;lower thermal expansion&#8221; as a 6106 advantage is reporting a rounding difference as if it were a property. If thermal movement governs your joint design, treat these alloys as identical and solve the problem in detail design.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>Electrical conductivity is genuinely higher<\/strong>, and it is the lean chemistry showing up in the numbers. At roughly 49% IACS, 6106 runs above 6061 (about 40\u201343%), which is why it turns up in bus bar, conductor rail, and heat sink work where the mechanical requirement is modest but the electrical one is not. Combined with ~190 W\/m\u00b7K thermal conductivity, that makes it a reasonable single-spec choice for parts that must carry both current and heat.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">The ~160 \u00b0C ceiling is a real limit, not a formality. Strength comes from Mg\u2082Si precipitates, and sustained exposure above roughly that temperature coarsens them permanently. There is no re-aging your way back once a part has been cooked.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">Why 6106 Is Classified as an Extrusion Alloy<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">This is the section most alloy write-ups skip, and it is the one that decides whether 6106 belongs on your drawing at all.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Extrudability is not a single property. It is a bundle of behaviors that together determine what a press can produce: how much pressure the alloy resists as it flows through the die, how fast it can be pushed before the surface tears, whether it fills thin and remote corners, how much the die deflects, and whether the finished surface looks clean enough to ship without masking the defects under paint. Alloy content pushes every one of those in the wrong direction, so a lean chemistry wins by default \u2014 and 6106 is lean.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">What that buys in practice:<\/p>\n\n\n\n<ul class=\"wp-block-list\">\n<li><strong>Thinner minimum walls.<\/strong> A section whose web has to come down to meet a weight target may simply not be fillable in 6061 at production speed, while running comfortably in 6106.<\/li>\n\n\n\n<li><strong>Higher complexity.<\/strong> Multi-void hollows, deep recesses, and fine detail are all easier. Stockists routinely note that shapes impossible in 6082 are routine in 6106.<\/li>\n\n\n\n<li><strong>Better surface.<\/strong> Lower flow stress means less die pickup and fewer surface defects, which matters directly when the finish is anodized rather than painted.<\/li>\n\n\n\n<li><strong>Higher line speed.<\/strong> Depending on the section, 6106 can run faster than 6061, which shows up in unit cost even when the billet price is the same.<\/li>\n<\/ul>\n\n\n\n<p class=\"wp-block-paragraph\">The trade is strength, discussed next.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">If you want the mechanics of the process itself, including what a mill needs from a drawing before quoting a profile, our <a href=\"https:\/\/premiumalu.com\/tr\/aluminyum-ekstruzyon-ozel-profillerini-kesfedin\/\">custom aluminum extrusion guide<\/a> covers it separately.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">6106 vs 6063 vs 6061 vs 6082<\/h2>\n\n\n\n<figure class=\"wp-block-image size-full\"><img decoding=\"async\" width=\"800\" height=\"600\" src=\"https:\/\/premiumalu.com\/wp-content\/uploads\/2025\/03\/6106-vs-6063-vs-6061-vs-6082.png\" alt=\"\" class=\"wp-image-10645\" srcset=\"https:\/\/premiumalu.com\/wp-content\/uploads\/2025\/03\/6106-vs-6063-vs-6061-vs-6082.png 800w, https:\/\/premiumalu.com\/wp-content\/uploads\/2025\/03\/6106-vs-6063-vs-6061-vs-6082-300x225.png 300w, https:\/\/premiumalu.com\/wp-content\/uploads\/2025\/03\/6106-vs-6063-vs-6061-vs-6082-768x576.png 768w, https:\/\/premiumalu.com\/wp-content\/uploads\/2025\/03\/6106-vs-6063-vs-6061-vs-6082-16x12.png 16w, https:\/\/premiumalu.com\/wp-content\/uploads\/2025\/03\/6106-vs-6063-vs-6061-vs-6082-600x450.png 600w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/><\/figure>\n\n\n\n<p class=\"wp-block-paragraph\">This comparison is where 6106 actually earns or loses a specification, and picking the right comparator matters \u2014 comparing only against 6061 makes 6106 look like a weaker version of something, rather than what it is.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Typical T6 values:<\/p>\n\n\n\n<figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td>M\u00fclkiyet<\/td><td><a href=\"https:\/\/premiumalu.com\/tr\/urun\/6106-aluminyum-alasim\/\" data-type=\"link\" data-id=\"https:\/\/premiumalu.com\/product\/6106-aluminum-alloy\/\">6106-T6<\/a><\/td><td><a href=\"https:\/\/premiumalu.com\/tr\/urun\/6063-aluminyum-alasim\/\" data-type=\"link\" data-id=\"https:\/\/premiumalu.com\/product\/6063-aluminum-alloy\/\">6063-T6<\/a><\/td><td><a href=\"https:\/\/premiumalu.com\/tr\/urun\/6061-aluminyum-alasim\/\" data-type=\"link\" data-id=\"https:\/\/premiumalu.com\/product\/6061-aluminum-alloy\/\">6061-T6<\/a><\/td><td><a href=\"https:\/\/premiumalu.com\/tr\/urun\/6082-aluminyum-alasim\/\" data-type=\"link\" data-id=\"https:\/\/premiumalu.com\/product\/6082-aluminum-alloy\/\">6082-T6<\/a><\/td><\/tr><tr><td>\u00c7ekme mukavemeti (MPa)<\/td><td>~290<\/td><td>~240<\/td><td>~310<\/td><td>~310<\/td><\/tr><tr><td>Akma mukavemeti (MPa)<\/td><td>~220<\/td><td>~215<\/td><td>~275<\/td><td>~260<\/td><\/tr><tr><td>Uzama (%)<\/td><td>~9<\/td><td>~12<\/td><td>~12<\/td><td>~10<\/td><\/tr><tr><td>Complex thin-wall extrusion<\/td><td>\u00c7ok iyi<\/td><td>M\u00fckemmel<\/td><td>\u0130yi<\/td><td>Adil<\/td><\/tr><tr><td>Anodized surface quality<\/td><td>\u00c7ok iyi<\/td><td>Best<\/td><td>\u0130yi<\/td><td>Adil<\/td><\/tr><tr><td>\u0130\u015flenebilirlik<\/td><td>\u0130yi<\/td><td>Orta d\u00fczeyde<\/td><td>\u0130yi<\/td><td>Orta d\u00fczeyde<\/td><\/tr><tr><td>Arc weldability<\/td><td>\u00c7ok iyi<\/td><td>\u00c7ok iyi<\/td><td>\u00c7ok iyi<\/td><td>\u0130yi<\/td><\/tr><tr><td>Typical work<\/td><td>Ladders, towers, rail stock, auto structures<\/td><td>Mimari d\u00f6\u015feme, pencere \u00e7er\u00e7eveleri<\/td><td>General structural, machined parts<\/td><td>Bridges, cranes, heavy frames<\/td><\/tr><\/tbody><\/table><\/figure>\n\n\n\n<p class=\"wp-block-paragraph\">The reading that matters: <strong>6106-T6 carries roughly 20% more tensile strength than 6063-T6 while staying much closer to it than to 6061 on the extrudability axis.<\/strong> That is the specific reason to specify it \u2014 a structural section that still needs to look good anodized, and needs to be more complicated than 6061 will reliably produce.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Where each alternative wins instead:<\/p>\n\n\n\n<ul class=\"wp-block-list\">\n<li><strong>6063<\/strong> when the part is architectural trim or window framing, the section is simple, the finish is the priority, and loads are low. It extrudes even more easily and finishes better.<\/li>\n\n\n\n<li><strong>6061<\/strong> when strength governs, when the part will be machined heavily, or when you want the widest stock coverage and engineers already know it. See our <a href=\"https:\/\/premiumalu.com\/tr\/6061-aluminyum-icin-eksiksiz-kilavuz\/\">6061 al\u00fcminyum rehberi<\/a>.<\/li>\n\n\n\n<li><strong>6082<\/strong> for heavy structural work \u2014 bridges, cranes, vehicle chassis \u2014 where its strength-to-toughness balance is the reason it is specified, accepting that complex thin sections are off the table. Compare <a href=\"https:\/\/premiumalu.com\/tr\/aluminyum-6082-t6da-ustalasmak-icin-eksiksiz-kilavuz\/\">6082-T6<\/a> before committing to a section.<\/li>\n\n\n\n<li><strong>6005<\/strong> is another thin-wall structural extrusion worth pricing alongside 6106 for structural tube and truss work; its <a href=\"https:\/\/premiumalu.com\/tr\/6005-aluminyum-alasimi-icin-temel-kilavuz\/\">properties and limits<\/a> differ enough to be worth a look.<\/li>\n<\/ul>\n\n\n\n<h2 class=\"wp-block-heading\">Uygulamalar<\/h2>\n\n\n\n<figure class=\"wp-block-image size-full\"><img decoding=\"async\" width=\"800\" height=\"600\" src=\"https:\/\/premiumalu.com\/wp-content\/uploads\/2025\/03\/Applications-and-Selection-Limits.png\" alt=\"\" class=\"wp-image-10647\" srcset=\"https:\/\/premiumalu.com\/wp-content\/uploads\/2025\/03\/Applications-and-Selection-Limits.png 800w, https:\/\/premiumalu.com\/wp-content\/uploads\/2025\/03\/Applications-and-Selection-Limits-300x225.png 300w, https:\/\/premiumalu.com\/wp-content\/uploads\/2025\/03\/Applications-and-Selection-Limits-768x576.png 768w, https:\/\/premiumalu.com\/wp-content\/uploads\/2025\/03\/Applications-and-Selection-Limits-16x12.png 16w, https:\/\/premiumalu.com\/wp-content\/uploads\/2025\/03\/Applications-and-Selection-Limits-600x450.png 600w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/><\/figure>\n\n\n\n<p class=\"wp-block-paragraph\">6106 shows up wherever a welded structural assembly needs to be light, extruded rather than machined, and held to tight dimensional repeatability.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>Ladders, towers, and masts.<\/strong> The classic application, and named first by nearly every stockist. Extension ladders and scaffold rails benefit from thin-wall hollow sections at high stiffness-per-weight, from clean surface finish on parts users handle, and from weldability. Rung-to-rail joints are welded, so the HAZ allowance below governs the joint design.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>Railway rolling stock.<\/strong> Extruded structural sections in body frames, floor supports, and interior framing. The combination of complex multi-void profiles, weldability, and fire and smoke behavior keeps 6xxx alloys dominant here, and 6106&#8217;s fill capability supports the integrated sections that replace multiple fabricated parts.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>Automotive structures.<\/strong> Crash boxes, bumper beams, subframe components, roof rails, and battery enclosure framing. Thin-wall capability drives mass reduction directly, and the higher conductivity matters where the enclosure is part of a thermal management path.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>Marine and offshore.<\/strong> Deck structures, gangways, masts, and superstructure framing. Worth stating plainly, though: good general corrosion resistance is not the same as marine-grade. Continuous seawater immersion or splash-zone service belongs to <a href=\"https:\/\/premiumalu.com\/tr\/5083-alumi%cc%87nyum-alasimlarinda-uzmanlasma-uzman-kilavuzu\/\">5xxx alloys<\/a> such as 5083-H116 or 5086-H116, which resist sensitization in a way high-magnesium-but-different 6xxx sections do not. Use 6106 above the waterline, not below it.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>Architecture and building.<\/strong> Structural curtain wall members, structural glazing profiles, and framing that carries real load rather than trim, where the same extrusion must satisfy both deflection limits and an appearance requirement.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>Thermal and electrical.<\/strong> Heat sinks, bus bars, conductor rail, and electrical enclosures, drawing on ~190 W\/m\u00b7K thermal conductivity and ~49% IACS electrical conductivity. Here the mechanical spec usually arrives second and the section is simple.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">Welding 6106<\/h2>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"800\" height=\"600\" src=\"https:\/\/premiumalu.com\/wp-content\/uploads\/2025\/03\/Welding-6106.png\" alt=\"\" class=\"wp-image-10649\" srcset=\"https:\/\/premiumalu.com\/wp-content\/uploads\/2025\/03\/Welding-6106.png 800w, https:\/\/premiumalu.com\/wp-content\/uploads\/2025\/03\/Welding-6106-300x225.png 300w, https:\/\/premiumalu.com\/wp-content\/uploads\/2025\/03\/Welding-6106-768x576.png 768w, https:\/\/premiumalu.com\/wp-content\/uploads\/2025\/03\/Welding-6106-16x12.png 16w, https:\/\/premiumalu.com\/wp-content\/uploads\/2025\/03\/Welding-6106-600x450.png 600w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/><\/figure>\n\n\n\n<p class=\"wp-block-paragraph\">106 is rated very good for arc welding. The difficulty is not joining it \u2014 it is what the arc does to the temper alongside the weld.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>The heat-affected zone loses strength.<\/strong> 6106 takes its strength from Mg\u2082Si precipitates locked in by heat treatment. A fusion weld reheats the adjacent metal through that same precipitation window without control, over-aging or dissolving what a furnace cycle built, so the zone beside the weld can lose up to half the parent strength. Lower heat input reduces that loss; it does not remove it. AWS D1.2 reflects this by directing designers to T4 or O properties for the heat-affected zone rather than T6 values, so the operating rule for 6106 is the same one used for every heat-treatable 6xxx extrusion: size the joint on reduced values, and confirm the figure with a qualification test where the load case matters.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>What helps:<\/strong><\/p>\n\n\n\n<ul class=\"wp-block-list\">\n<li><strong>Move the weld.<\/strong> The soft zone runs roughly 15\u201325 mm from the weld centerline, so keeping welds clear of peak bending stress is the cheapest fix.<\/li>\n\n\n\n<li><strong>Oversize locally.<\/strong> One wall size up on a tube usually recovers the whole welded loss for very little weight.<\/li>\n\n\n\n<li><strong>Fasten instead.<\/strong> A bolted joint keeps full parent T6 strength.<\/li>\n\n\n\n<li><strong>Weld in T4, then age.<\/strong> Welding before artificial aging recovers appreciably more than welding after it, and a low-temperature cycle on an already-T6 weldment adds almost nothing. We do not run aging in-house, so build it into the schedule.<\/li>\n<\/ul>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>Filler.<\/strong> ER4043 suits general fabrication; ER5356 where you need more as-welded strength or a closer color match after anodizing. Our <a href=\"https:\/\/premiumalu.com\/tr\/basari-icin-aluminyum-kaynak-teli-hakkinda-uzman-ipuclari\/\">al\u00fcminyum kaynak teli k\u0131lavuzumuzda<\/a> covers the selection, and the <a href=\"https:\/\/premiumalu.com\/tr\/6061-aluminyum-kaynak-tekniklerinde-ustalasma\/\">6061 welding guide<\/a> covers procedure control and joint-strength qualification.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">Machining, Forming, and Surface Finishing<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>\u0130\u015fleme.<\/strong> 6106 machines well in T6 with sharp tools and adequate clearance; the softer O and T4 conditions are more prone to built-up edge and smearing, so the &#8220;gummy&#8221; reputation attaches to those rather than to the T6 condition people actually machine. In general machining ranking, 6061 still performs better, so where a part is mostly chips rather than mostly extrusion, 6061 remains the better ask.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>\u015eekillendirme.<\/strong> Do it before final aging. T4 is the practical forming condition for bending and shaping; T6 tolerates only limited cold work, and attempting tight bends there invites cracking along the outer fiber. Springback is moderate and is better controlled by die design than by alloy substitution. Remember that any heavy local heating during straightening will soften the area in the same way a weld does.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>Eloksal.<\/strong> One of 6106&#8217;s real advantages. Low iron and copper give consistent clear and colored anodic films, and the good as-extruded surface means less mechanical prep before the tank. The practical caution is that a 6106 section welded together will show the weld and its HAZ as a visible band after anodizing unless the filler and procedure are chosen for appearance; our <a href=\"https:\/\/premiumalu.com\/tr\/eloksal-renklendirme-ipuclarini-ve-kalite-bilgilerini-kesfedin\/\">anodizing guide<\/a> explains why most visible failures start with alloy selection and surface preparation rather than with the anodizing itself.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>Corrosion.<\/strong> Good general atmospheric corrosion resistance, typical of the 6000 series, and better than many users expect in industrial atmospheres. It is not immune to intergranular attack in aggressive conditions, and it does not belong in continuous immersion or the splash zone. Powder coating or anodizing extends service life substantially; for marine immersion, move to 5xxx rather than upgrading the finish.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">Standards and Procurement Documentation<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">Getting the paperwork right matters as much as getting the alloy right, because it is what determines whether the section you receive is the one you specified.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>Specify the standard and the temper together.<\/strong> &#8220;6106-T6&#8221; alone leaves too much open. A complete line item names the alloy, temper, product form, governing specification, applicable dimensional tolerance, and wall-thickness class. For extruded product that means <strong>ASTM B221<\/strong> veya <strong>EN 755-2<\/strong> (with <strong>EN 573-3<\/strong> for composition analysis and <strong>GB\/T 3190<\/strong> for Chinese mill supply). Confirm availability before quoting if a drawing calls for 6106 against a rolled plate or sheet specification \u2014 a mismatch discovered after award costs far more than a question asked early.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\"><strong>Documents worth requesting:<\/strong><\/p>\n\n\n\n<figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td>Dok\u00fcman<\/td><td>Sa\u011flad\u0131\u011f\u0131 \u00f6zellikler<\/td><\/tr><tr><td>Mill test certificate (MTC)<\/td><td>Heat-specific composition and actual mechanical values for the supplied lot<\/td><\/tr><tr><td>EN 10204 3.1 certificate<\/td><td>Mill-independent statement that values were verified against the order<\/td><\/tr><tr><td>SGS chemical or mechanical report<\/td><td>Third-party verification where the project requires it<\/td><\/tr><tr><td>SGS dimensional inspection<\/td><td>Verification of critical profile dimensions against the drawing<\/td><\/tr><\/tbody><\/table><\/figure>\n\n\n\n<p class=\"wp-block-paragraph\">The distinction to hold onto: the figures in this article are <strong>tipiktir<\/strong> values for orientation. The numbers that bind are the standard minimums and the MTC values for the specific lot. When those disagree, the MTC wins.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Also worth confirming before placing an order: the wall thickness class, since it drives the minimum mechanical values; the temper route, T5 versus T6, since it changes both cost and properties; and whether the drawing intends any post-extrusion aging after forming or welding, since that step belongs in the schedule rather than discovered mid-fabrication.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">When to Choose 6106 \u2014 and When Not To<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">Choose 6106 when:<\/p>\n\n\n\n<ul class=\"wp-block-list\">\n<li><strong>The section is the constraint<\/strong>, not the alloy number \u2014 thin walls, multiple voids, tight tolerances, or details that 6061 will not fill reliably at production speed.<\/li>\n\n\n\n<li><strong>You need more strength than 6063 and better finish than 6061<\/strong>, particularly where the same extrusion is structural and visible.<\/li>\n\n\n\n<li><strong>The part will be welded and moderately loaded<\/strong>, with room to place joints away from peak stress or to oversize locally. Every 6xxx behaves this way; plan for it.<\/li>\n\n\n\n<li><strong>Weight per metre is being driven down<\/strong> through wall thickness rather than through alloy substitution.<\/li>\n\n\n\n<li><strong>The part also conducts<\/strong> \u2014 bus bar, heat sink, conductor rail \u2014 where roughly 49% IACS is an advantage 6061 cannot match.<\/li>\n<\/ul>\n\n\n\n<p class=\"wp-block-paragraph\">\u015eu durumlarda ba\u015fka yerlere bak\u0131n:<\/p>\n\n\n\n<ul class=\"wp-block-list\">\n<li><strong>Peak strength governs the design.<\/strong> Step up to <a href=\"https:\/\/premiumalu.com\/tr\/urun\/6061-aluminyum-alasim\/\">6061-T6<\/a> or 6082-T6.<\/li>\n\n\n\n<li><strong>A welded joint must retain full T6 strength.<\/strong> No 6xxx alloy does this. Either redesign so the weld is not the governing location, or consider whether a non-heat-treatable 5xxx grade suits the load case better.<\/li>\n\n\n\n<li><strong>The service is continuous seawater immersion or splash zone.<\/strong> Move to 5083-H116 or 5086-H116.<\/li>\n\n\n\n<li><strong>The part is decorative architectural trim with low load.<\/strong> 6063 extrudes more easily and anodizes better, and it costs less. See our <a href=\"https:\/\/premiumalu.com\/tr\/6063-aluminyum-ekstruzyonlar-icin-uzman-ipuclari\/\">6063 ekstr\u00fczyon k\u0131lavuzu<\/a>.<\/li>\n\n\n\n<li><strong>Service runs continuously above roughly 160 \u00b0C.<\/strong> Precipitation coarsening is permanent.<\/li>\n<\/ul>\n\n\n\n<h2 class=\"wp-block-heading\">Sonu\u00e7<\/h2>\n\n\n\n<p class=\"wp-block-paragraph\">6106 is a 6xxx extrusion alloy that trades peak strength for how far it can be pushed through a die \u2014 roughly 20% stronger than 6063-T6 while still filling thin-wall and multi-void sections that 6061 cannot produce reliably. Two specification traps drive most failures with it: ordering it against a rolled plate or sheet standard instead of ASTM B221 or EN 755-2, and sizing welded joints on T6 parent values when fusion welding removes up to half the local strength.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">We supply <a href=\"https:\/\/premiumalu.com\/tr\/urun\/6106-aluminyum-alasim\/\">6106<\/a> as profile, bar, tube, and wire in O, T4, T5, and T6, quoted to ASTM B221 or EN 755-2 with the wall-thickness class stated, and we handle CNC machining, welding, laser cutting, and anodizing in-house. Post-weld aging is a separate mill step we do not run ourselves, so build it into the schedule, and every order carries an MTC.<\/p>\n\n\n\n<p class=\"wp-block-paragraph\">Send us the drawing, the standard, and the temper route, and we will confirm available wall thicknesses, tolerances, and documentation before you commit.<\/p>\n\n\n\n<h2 class=\"wp-block-heading\">S\u0131k\u00e7a Sorulan Sorular<\/h2>\n\n\n\n<h3 class=\"wp-block-heading\">How does 6106 pricing compare with 6063 and 6061?<\/h3>\n\n\n\n<p class=\"wp-block-paragraph\">The grade matters less than how the part is bought. 6106 is a narrower designation with less mill stock than 6063, so form, temper and order quantity move the number more than the alloy choice does. Send the section, temper and annual volume, and we will quote the actual lot rather than a list price.<\/p>\n\n\n\n<h3 class=\"wp-block-heading\">What is the minimum order quantity for 6106?<\/h3>\n\n\n\n<p class=\"wp-block-paragraph\">Stocked profiles ship from standard pack quantities. Anything outside the stocked range is a low-MOQ custom run, so the practical minimum depends on the form, the temper and whether a heat is available. Tell us the specification and quantity and we will confirm what ships from stock and what has to be produced.<\/p>\n\n\n\n<h3 class=\"wp-block-heading\">What lead time should I expect for 6106 extrusions?<\/h3>\n\n\n\n<p class=\"wp-block-paragraph\">Plan on roughly 10\u201360 days, depending on whether the profile is stocked. Stocked sections ship in days; a new die adds design, fabrication and trial time before the first extruded length. Confirm the section against your build schedule early, because the die is on the critical path.<\/p>","protected":false},"excerpt":{"rendered":"<p>6106 is a medium-strength, heat-treatable 6xxx extrusion alloy. Its defining property is extrudability: it flows into thin, complex sections that the stronger 6xxx grades will not fill. It carries less magnesium and silicon than 6061, and that leaner chemistry is the point \u2014 it can be extruded into thinner walls and more complicated cross-sections than [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":10644,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_seopress_titles_title":"6106 Aluminum Guide: Composition, Strength, Extrusions","_seopress_titles_desc":"6106 aluminum guide: composition, T6 strength, tempers, and the extrudability that sets it apart from 6061 \u2014 with direct comparisons to 6063, 6082, and 6005.","_seopress_robots_index":"","_seopress_robots_follow":"","_seopress_robots_imageindex":"","_seopress_robots_snippet":"","_seopress_robots_primary_cat":"","_seopress_robots_breadcrumbs":"","_seopress_robots_freeze_modified_date":"","_seopress_robots_custom_modified_date":"","_seopress_robots_canonical":"","_seopress_social_fb_title":"","_seopress_social_fb_desc":"","_seopress_social_fb_img":"","_seopress_social_fb_img_attachment_id":0,"_seopress_social_fb_img_width":0,"_seopress_social_fb_img_height":0,"_seopress_social_twitter_title":"","_seopress_social_twitter_desc":"","_seopress_social_twitter_img":"","_seopress_social_twitter_img_attachment_id":0,"_seopress_social_twitter_img_width":0,"_seopress_social_twitter_img_height":0,"_seopress_redirections_value":"","_seopress_redirections_enabled":"","_seopress_redirections_enabled_regex":"","_seopress_redirections_logged_status":"","_seopress_redirections_param":"","_seopress_redirections_type":0,"_seopress_analysis_target_kw":"","footnotes":""},"categories":[177],"tags":[],"class_list":["post-8323","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-5000_6000-series-aluminum"],"_links":{"self":[{"href":"https:\/\/premiumalu.com\/tr\/wp-json\/wp\/v2\/posts\/8323","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/premiumalu.com\/tr\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/premiumalu.com\/tr\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/premiumalu.com\/tr\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/premiumalu.com\/tr\/wp-json\/wp\/v2\/comments?post=8323"}],"version-history":[{"count":4,"href":"https:\/\/premiumalu.com\/tr\/wp-json\/wp\/v2\/posts\/8323\/revisions"}],"predecessor-version":[{"id":10652,"href":"https:\/\/premiumalu.com\/tr\/wp-json\/wp\/v2\/posts\/8323\/revisions\/10652"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/premiumalu.com\/tr\/wp-json\/wp\/v2\/media\/10644"}],"wp:attachment":[{"href":"https:\/\/premiumalu.com\/tr\/wp-json\/wp\/v2\/media?parent=8323"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/premiumalu.com\/tr\/wp-json\/wp\/v2\/categories?post=8323"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/premiumalu.com\/tr\/wp-json\/wp\/v2\/tags?post=8323"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}