What Is 7075-T7451?

7075-T7451 is the 7075 thick-plate temper that sits between peak strength and maximum corrosion resistance. T7451 means the plate was solution heat treated, water quenched, stretched 1.5–3% to remove residual stress, then overaged — but not overaged as far as T7351. That half-step is the whole point of the temper: it keeps more strength than T73 while staying far more resistant to stress-corrosion cracking than T651.

It is a plate temper, not a bar or extrusion temper. The stretch is what makes thick plate machine flat, and the overaging is what keeps a thick section from cracking under sustained tension in humid or chloride-bearing service. Bar and extrusion equivalents carry their own designations — T73511 for extruded bar, for example — and the numbering matters on a purchase order because the properties move with it.

Four tempers form the set you are choosing from: T651, T7651, T7451 and T7351. They are not four different alloys or four quality levels. They are four stops on one continuous axis — how far the aging treatment is pushed past the peak.

Understanding the T7x Ladder

Peak-aged 7075 is an alloy with a corrosion problem. T6 and its stretched plate version T651 give the highest strength available in wrought aluminum, and in a humid or chloride environment they will crack under sustained tensile load — a failure mode no coating removes. The industry’s answer was to overage: age past the peak on purpose, accepting lower strength in exchange for a microstructure that resists cracking.

Every one of the four tempers is a different answer to "how far past the peak". The "51" suffix is constant across them: it means the plate was stretched after quenching, which thick plate needs for machining stability.

T651 — Peak Strength, No Overage

The baseline. Highest strength of the four, poorest resistance to stress-corrosion cracking. Correct when the service environment is dry, protected, or the part never sees sustained tensile stress in the short-transverse direction. This is the temper most stock 7075 plate ships in, and the one most general machining work is written against.

T7651 — Slight Overage, Aimed at Exfoliation

T7651 gives up roughly 3.5% of T651’s tensile strength. Its purpose is narrower than the other two overaged stops: it targets exfoliation corrosion, the layer-by-layer delamination that attacks plate edges and machined surfaces, rather than stress-corrosion cracking in the short-transverse direction. A T7651 plate is materially better than T651 in an exposed edge condition, and only modestly better in SCC.

That distinction is worth holding onto, because it breaks the tidy story. T76 and T73 answer two different failure modes, so rank these tempers by what they protect against — not by how far they are overaged.

T7451 — The Middle Stop

T7451 is a fuller overage than T7651 but a lighter one than T7351, and it is the temper this article is built around. It gives up about 8% of T651’s tensile strength, and in exchange it delivers SCC resistance close to T73’s — which is to say, in a different class from T651.

The way to hold it in mind: T7451 is T7351 that has not been overaged as far. You get roughly 6% more tensile strength than T7351 and give up a little of its corrosion margin. For a thick section that must carry real load in a wet environment, that is often the better trade.

T7351 — Full Overage

The most overaged of the four. Roughly 13% below T651 in tensile strength, and the most resistant to stress-corrosion cracking — which is why it is the default for thick aircraft structure in the short-transverse direction: wing ribs, spar caps, frames, bulkheads, and defence hardware where a crack is not an acceptable outcome at any strength level.

Four precision-machined 7075 aluminum plate specimens arranged side-by-side illustrating the overage ladder from T651 to T7351
The 7075 plate overage ladder: advancing past peak strength trades tensile strength for stress-corrosion and exfoliation resistance.

7075-T7451 Mechanical Properties

TemperTensileYieldUzamavs T651 (tensile)
T651572 MPa503 MPa11%baseline
T7651552 MPa490 MPa11%−3.5%
T7451524 MPa469 MPa11%−8.4%
T7351496 MPa434 MPa12%−13.3%

Typical plate values to ASTM B209 and the matching AMS plate specifications (AMS 4078 for T7351); the acceptance range for each temper and gauge is set by that specification. Thicker sections run slightly lower because the quench rate falls with thickness — take the numbers off the certificate for the gauge you are buying.

Read the percentage column, not the absolute one. On paper 524 MPa against 572 looks like a real loss. In design terms, the question is whether you need the top 8% of the strength range — and if the part lives in humidity, salt, or chloride, the answer is usually that you do not, because T651’s extra 8% comes with a cracking mode that does not announce itself.

For a specifier: T7451 keeps roughly 91% of the tensile strength of T651 and most of the SCC resistance of T7351. That is an unusually good position on the curve, which is why it exists as a separate temper rather than being folded into one of its neighbours.

Where Each Stop Is Used

T7451 — Load-Bearing Structure in Wet Service

Large machined structural components, aircraft fittings that see both load and moisture, long-stored tooling and fixtures where dimensional stability over years matters as much as strength. The common thread is a part that has to carry a calculated load and cannot be relied on to stay dry for its whole life.

T7351 — Thick Sections Where Cracking Is Unacceptable

Wing ribs, spar caps and spar webs, frames, bulkheads, heavy defence structure. These are thick sections loaded in the short-transverse direction, which is exactly where peak-aged 7075 is weakest against SCC. The 13% strength sacrifice is the price of not having a crack initiate in a part nobody can inspect from the inside.

T7651 and T651 — Exposed Edges and Dry Service

T7651 for plate whose machined edges and surfaces will be exposed to weather and where exfoliation is the concern. T651 for dry, protected, strength-critical parts — the general machining, mould and automation work that most 7075 plate actually goes into.

T7451 vs T7351 vs T7651 vs T651 — How to Choose

MülkiyetT651T7651T7451T7351
Tensile572 MPa552 MPa524 MPa496 MPa
SCC direnciZayıfOrta düzeydeGood, near T73En iyi
Exfoliation resistanceZayıfİyiİyiİyi
İşleme stabilitesiGood (stretched)İyiİyiİyi
İçin en iyisiDry, protected, peak strengthExposed edges, exfoliation riskLoad plus moistureThick sections, crack-critical
Macro comparison of two thick 7075 aluminum blocks under short-transverse tensile loading showing T651 micro-cracking versus T7451 crack immunity
Short-transverse (ST) tensile loading in thick plate: T651 carries high stress-corrosion cracking risk along rolling grain boundaries; T7451 and T7351 provide crack immunity.

Start with two questions, in this order. Is there sustained tensile stress in the short-transverse direction? If yes, T651 is out — move to T7451 or T7351. Is the section thick enough that a crack could not be found before it mattered? If yes, T7351. If the part is machinable, load-bearing but moderately sectioned, T7451 is usually the better trade, and T7651 only enters when exfoliation on exposed edges is the specific worry.

When T7451 Is the Right Call

Two conditions together: the part carries a calculated load, and it cannot be guaranteed dry for its service life. Aircraft fittings, marine-adjacent structure, long-life tooling in humid plants. Under those conditions T7451’s 8% strength sacrifice buys a corrosion margin that T651 does not have, at a strength T7351 cannot reach.

When T7351 Fits Better

When the section is thick and the failure mode is the one you cannot inspect. Short-transverse loading in heavy plate, defence structure, anything where a crack initiating inside the part is worse than 60 MPa of lost strength. Do not use T7451 here to save strength — the trade runs the wrong way.

Working With 7075-T7451 — Machining, Corrosion, Finishing

İşleme (Talaşlı İmalat): the stretch in the "51" is what makes this work. A T7451 plate machined into a thin-walled part stays flat where a T6 plate would move as material is removed. Cut it with sharp carbide and good coolant; 7075 at this hardness is not forgiving of a rubbing cutter.

Korozyon koruması: T7451 resists SCC far better than T651 but is still a copper-bearing 7xxx alloy with modest general corrosion resistance. Anodize (Type II or III) or apply a conversion coating on exposed surfaces, and never rely on the overaged temper as a substitute for a finish in salt service.

Yüzey işleme: anodizing is routine, though 7075 takes a darker, less uniform coating than 6xxx and hard anodize is more common than decorative anodize on this alloy. Mask or ream critical bores after coating, since the oxide layer changes dimensions.

Kaynak: not a welding alloy. 7075 in any temper is generally not fusion welded for structural service; design for mechanical fastening or move to a weldable alloy if the joint is structural.

Artılar ve Sınırlamalar Bir Bakışta

BoyutAvantajBedeli
Güç524 MPa tensile — above T7351, close to T6518% below T651’s peak
SCC direnciClose to T73, far better than T651Not equal to T7351 in the worst short-transverse case
İşleme stabilitesiThe stretch keeps thin-walled parts flatThick plate needs stretching capacity, which limits supply
Corrosion, generalBetter than T651 in wet serviceStill needs a coating in salt or chloride
ExfoliationİyiT7651 is the temper aimed specifically at this
Kaynaklanabilirlik—Not a fusion-welding alloy in any temper

Sonuç

7075-T7451 is not "a stronger T7351" or "a safer T651". It is a deliberate point on one axis: about 8% below peak strength, with most of the stress-corrosion resistance that costs T7351 another 5 points more. For thick plate that carries load and cannot be kept dry, that is usually the best trade available — and it is why the temper exists at all.

We supply 7075-T7451 and T7351 plate, along with T651 and T7651, with a Mill Test Certificate on every order. Thick overaged plate depends on stretching capacity, so lead time is quoted against the gauge and size you need.

Send us the part drawing with the temper, thickness and service environment, and we will confirm which stop on the ladder fits and quote against it.

Sıkça Sorulan Sorular

Is T7451 stronger than T7351?

Yes. On plate to ASTM B209, T7451 runs about 524 MPa against 496 for T7351 — roughly 6% more on tensile, and about 8% more on yield — because it is overaged less. It gives up some SCC resistance for that; both far exceed T651.

Can I use T7451 instead of T651?

Only if the environment justifies it. T7451 costs about 8% of T651’s tensile strength. Take that trade when the part sees sustained tensile stress in humidity or chloride, where T651 is SCC-sensitive.

What does the "51" in T7451 mean?

Stress relieved by stretching, 1.5–3% after quenching. It is what makes thick plate machine flat. Without the stretch the temper would be T74, which is not a plate product.

Minimum sipariş ve teslim süresi nedir?

Low MOQ, typically 10–60 days depending on temper, thickness and size. Overaged thick plate depends on stretching capacity, so confirm the gauge before a firm date is quoted.

David Huang

David Huang, Çin'in alüminyum alaşım endüstrisinde son derece saygın bir uzmandır ve gelişmiş alüminyum alaşımlarının geliştirilmesi, üretimi ve uygulanması konusunda on yılı aşkın bir deneyime sahiptir. Havacılık, otomotiv ve inşaat dahil olmak üzere çeşitli sektörlerde önde gelen küresel şirketlere başarılı bir şekilde proje çözümleri ve teknik uzmanlık sunma konusunda kanıtlanmış bir geçmişe sahiptir. David ayrıca Çin'deki birçok büyük alüminyum üreticisinin güvenilir danışmanıdır.

7/24 Hizmet | 10 Dakika İçinde Yanıt!

Daha fazla katalog, detay ve fiyat teklifi için lütfen doğrudan bizimle iletişime geçin!

WhatsApp Telefon