2618 aluminum bar is a heat-treatable Al-Cu-Mg-Ni alloy (EN AW-2618 / AlCu2Mg1.5Ni, UNS A92618) for parts that stay strong when hot — pistons, compressor rotors and high-temperature structural parts. Round bar is supplied from 10 mm to 500 mm; square and flat bar on request. The standard temper is T61, not T6: it is aged at a higher temperature so the material does not over-age and soften in service at 150–250 °C.

形式: round bar 10–500 mm; square / flat on request; length 1000–6000 mm
状态: T61 / T6511 / T4 / T4511 / O
质量文件: 每笔订单均附有MTC报告

What Is 2618 Aluminum Bar?

2618 is a heat-treatable Al-Cu-Mg-Ni alloy (EN AW-2618 / AlCu2Mg1.5Ni, UNS A92618) used for parts that stay strong when hot — pistons, compressor rotors and high-temperature structural parts. Its deliberate iron and nickel content forms a dispersion that resists coarsening, which is why it holds strength to roughly 250 °C where ordinary age-hardening alloys have already over-aged. Bar is supplied as extruded round bar; the standard temper is T61, not T6. Metallurgy and equivalents: 2618 铝合金.

Bar Forms & Sizes

Round bar is the form we hold and quote most often. Square and flat bar are available on request against your section.

形式 Diameter / side (mm) 长度(毫米) 可用性
圆棒,挤压 10 – 500 1000 – 6000(定尺切割) Standard range
方棒 Quoted to section 1000 – 6000 按需提供
扁棒 Quoted to section 1000 – 6000 按需提供

Other 2618 forms — sheet, plate, tube, forging stock and wire — are described on the 合金页面. For bar in other alloys, see the 铝合金棒材系列.

状态、性能与选型

脾气 条件 抗拉强度 (MPa) 屈服强度 (MPa) 伸长率 适用场合
T61 Solution treated, artificially aged at elevated temperature ≥ 400 ≥ 310 ~8% The standard for 2618: pistons, hot tooling, heat-exposed structure
T6511 As T61, stress relieved by stretching and straightened ≥ 400 ≥ 310 ~8% Precision machining of bar where the part must not move
T4 / T4511 固溶处理,自然时效 按MTC Bar formed after delivery; low enquiry volume
O 退火 ~200 ~100 ~14% Machining stock before ageing, forming

Values are typical for 2618 and confirmed against the MTC for the lot. Hardness is roughly 115 HB in T61 and 55 HB in O. Density 2.70 g/cm³.

Why T61, not T6

On 6061 or 6082 the default is T6. On 2618 it is T61, and the difference is the ageing temperature, not an extra process step. T61 is aged at a higher temperature than a standard T6, which deliberately over-ages the alloy slightly: peak room-temperature strength is traded for stability, so the material does not continue to over-age and soften in service at 150–250 °C. That is exactly the range pistons and hot tooling live in.

Practical consequence: if a drawing for a piston or hot fixture specifies 2618-T6, question it. T6 can be quoted, but it is rarely what the application needs and it is not the temper the industry writes on 2618. T6511 is the same T61 condition with the bar stretched after quenching and then straightened — strength unchanged, residual stress removed, so long machined parts stay straight.

The same designation rule as other extrusions applies: T651 is rolled plate, not bar. Extruded bar is stress relieved as T6511. A bar certificate showing T651 is a designation error.

现货或按订单生产。. 这些状态并非在每个厚度和截面中都有库存。有库存的组合可直接发货,无最小起订量。由于状态范围较广,其余按订单生产并设有 MOQ——请告知我们状态、尺寸和数量,我们将确认适用哪种方式并报价。.

化学成分

要素 规格 要素 规格
铜 (Cu) 1.9 – 2.7 镁(Mg) 1.3 – 1.8
镍 (Ni) 0.9 – 1.2 铁(Fe) 0.9 – 1.3
硅 (Si) 0.10 – 0.25 钛 (Ti) 0.04 – 0.10
锰 (Mn) 0.15 最大值 铬 (Cr) 最大 0.10
锌 (Zn) 0.15 最大值 其他元素,单项/总计 0.05 / 0.15

Weight percent; aluminum is the balance. The nickel and iron are intentional, not impurities — they form the intermetallic dispersion that gives 2618 its hot strength.

应用

Engine pistons and piston crowns, compressor impellers and rotors, high-temperature structural brackets, helicopter rotor components, plastic injection moulds and hot fixtures, automotive connecting rods and other engine parts machined to tight tolerance. For the other common piston alloy, see 4032 铝合金.

Working Limits — Corrosion and Welding

Two limits belong on the enquiry rather than in the workshop:

  • 腐蚀: with 1.9–2.7% copper, 2618 has only fair corrosion resistance — below the 5xxx and 6xxx families. It is not suitable for marine or chemical exposure without protection. Hard anodizing or a conversion coating can be evaluated, though anodizing response is moderate because of the intermetallic phases.
  • 焊接: fusion welding is not recommended. High copper content makes 2618 susceptible to hot cracking in TIG and MIG, so arc welding should not be used for structural joints. Mechanical fastening or press-fit is the usual assembly route; friction stir welding may be viable in controlled production.

质量文件

Every order ships with an MTC issued by Linsy after production, reporting composition, mechanical results and the temper designation. Third-party testing is available on request at additional cost. Production runs under ISO 9001, ISO 14001 and ISO 45001 certified systems.

如何指定与询价

  1. 脾气 — T61, T6511, T4/T4511 or O
  2. 规格 ——圆棒直径,或方棒和扁棒的边长尺寸
  3. 长度 ——定尺长度,或若您自行切割则为不定尺
  4. 数量 ——件数或重量
  5. 直线度和公差 ——仅在具体数值至关重要时提供
  6. 目的地与包装 ——发货港口及任何标记要求

销售团队将确认该确切组合的库存或定制交期。.

为什么选择 Linsy

Shenzhen-based aluminum factory, more than 20 years in the industry, supplying 1000–8000 series alloys in standard specifications and custom sizes. 2618 round bar in T61 and T6511, with square and flat sections quoted on request; MTC with every order; low-MOQ custom production; typical custom lead time 10–60 days.

相关资源

2618 Aluminum Bar FAQ

Q: Do you supply 2618 bar in T6?
A: T6 can be quoted, but it is rarely what a 2618 application needs and it is not the temper the industry specifies. T61 is aged at a higher temperature specifically so the part keeps its strength at 150–250 °C. If your drawing says 2618-T6, tell us the service temperature and we will confirm what to order.

Q: Can you supply square or flat 2618 bar?
A: On request. Round bar from 10 mm to 500 mm is the standard range; square and flat sections are quoted to your dimensions and quantity. Send the section, length and quantity.

Q: Is T6511 different from T61 in strength?
A: No — both are ≥400 MPa tensile and ≥310 MPa yield. T6511 is stretched after quenching to remove residual stress and then straightened, so long machined parts do not move. Choose it for precision machining, T61 for everything else.

Q: Can 2618 bar be welded?
A: Fusion welding is not recommended — the copper content causes hot cracking in TIG and MIG. Mechanical fastening or press-fit is the usual route for assembly.