What Is 8009 Aluminum?

8009 aluminum is one of the 8xxx grades — the series that carries iron rather than copper, magnesium or zinc as its main addition — and it exists for one job: parts that have to carry load while running hot, usually between 150 °C and 300 °C. That is the range where 6061 and 2024 have already given up most of the strength their heat treatment gave them.

Its strength does not come from heat treatment at all. It comes from a very large number of fine particles — iron, silicon and vanadium, mixed into the metal while it is being made. That is the whole difference between 8009 and the alloys most buyers know. The metal is made from powder that is cooled extremely fast instead of being cast into a solid block the usual way, and that fast cooling is what keeps the particles fine enough to do their job.

The cost of that advantage sits on the buying side, not the engineering side. Very few plants can make the powder, so the material is not a catalogue item. It comes in two states rather than a ladder of tempers. And the aerospace specification written for it covers sheet only, which means anything thicker or in a different shape has to be ordered against a drawing instead of a standard. Once the alloy fits your temperature, what is left is working out the state it arrives in.

Why 8009 Holds Its Strength Where 6061 and 2024 Soften

6061 and 2024 get their strength from heat treatment, and heat treatment is undone by heat. From about 150 °C upward, the structure that made them hard gradually comes apart and the strength leaves with it. A 6061-T6 bracket that is comfortably within limits on the bench can be badly over-stressed at 200 °C, and nothing in the room-temperature datasheet warns you.

8009 works differently. The particles that give it strength are already in the metal and are stable at temperature: they do not grow, and they do not dissolve back into the aluminium. Heat the part and those particles go on holding the metal back from stretching, the same way they did when it was cold.

That is why the strength falls away gradually instead of dropping off a cliff. How much of it is left, and for how long, is what the table below shows.

Polished metallurgical specimen mounts comparing precipitate coarsening in 6061/2024 against stable dispersoid particles in 8009 aluminum at elevated temperatures
Microstructural comparison under sustained heat: conventional precipitation hardening softens above 150 °C, while 8009 dispersoids remain stable up to 300 °C.

8009 Aluminum Properties at Room and Elevated Temperature

PropertyValueBasis
Density2.92 g/cm³Typical
Tensile strength, room temperature450 MPaTypical
Yield strength, room temperature385 MPaTypical
Elongation~15%Typical
Tensile modulus90 GPaTypical
Hardness~140 HBTypical
Thermal conductivity~115 W/m·KTypical
Thermal expansion~19.0 µm/m·°CTypical

At room temperature, 8009 takes about 450 MPa before it breaks and 385 MPa before it stops springing back. For scale, 6061-T6 — the alloy most workshops know best — takes 310 MPa and 276 MPa on the same two measures, and 7075-T6 takes 572 MPa and 503 MPa. So 8009 is stronger than 6061 cold and weaker than 7075, which means room temperature is not the reason to buy it. Two other numbers matter more in practice. Density is 2.92 g/cm³, about 8% heavier than 6061 because of the iron, but still well under half the weight of steel. Hardness around 140 HB is close to 7075, so a shop that already machines 7075 will not be surprised by how it cuts.

The numbers at temperature are the reason the alloy exists.

TemperatureTensile strength after 1,000 hYield strength after 1,000 h
100 °C410 MPa370 MPa
150 °C380 MPa350 MPa
200 °C350 MPa310 MPa
250 °C310 MPa275 MPa
300 °C270 MPa240 MPa

At 200 °C the alloy still carries 350 MPa after a thousand hours at temperature — about 78% of what it does cold. At 250 °C it holds 310 MPa, and at 300 °C it still holds 270 MPa, which is a little below where 6061-T6 starts out at room temperature. The drop from 200 °C to 300 °C is steeper than the drop from room temperature to 200 °C, and that is the practical reading: 200–300 °C is the working window, and the top half of it needs more safety margin than the bottom half.

These are published typical values, not the minimums a specification guarantees. Ask the supplier for the values that apply to the heat you are actually being offered, and write the number you designed to into the purchase order rather than leaving it implied.

Tempers and Product Forms — What AMS 4308 Actually Covers

AMS 4308 is the aerospace material specification for this alloy, published by SAE International. It fixes the chemistry, the state and the strength figures the material has to meet, and it is the document an inspector works from when the material arrives. When a drawing says "AMS 4308", that is what the supplier is promising.

The chemistry comes down to six rows, and they are the ones worth checking on a certificate.

ElementRange (wt%)What it does
Iron (Fe)8.4 – 8.9The main addition; forms the particles that hold strength at temperature
Silicon (Si)1.7 – 1.9Works with the iron and vanadium to form those particles
Vanadium (V)1.1 – 1.5Keeps those particles stable when the part runs hot
Zinc (Zn)0.25 maxImpurity — this is the row that catches a wrong certificate
Oxygen (O)0.30 maxThe fingerprint of the powder route; an ingot-cast alloy would not carry a limit like this
AluminiumBalanceThe remainder

These are published typical limits, consistent with the 8.6Fe – 1.8Si – 1.3V chemistry named in AMS 4308B. Ask for the certified values for the batch you are quoting.

O (Annealed)

O is the softened state. The metal is heated and cooled slowly on purpose so it can be formed — bent, rolled or pressed into shape — and it gives up strength to do it. Buy O when the part still has to be shaped after you receive it, and plan on accepting lower strength figures until the forming is finished.

H112 / F (As-Fabricated)

H112 — often written F, for as-fabricated — is the state the material is in when it leaves the mill after being worked hot, with no further treatment applied. It is the default structural condition and the one the AMS 4308 title names, because there is no aging step to add or skip: the strength the alloy has is the strength the process produced.

The form question is where most purchase orders go wrong.

Physical product forms of 8009 aluminum comparing AMS 4308 specification sheets with custom ordered bar and heavy plate
8009 product forms: AMS 4308 covers rolled sheet only; plate, bar, and custom extrusions require technical agreements on the PO.
FormCovered byWhat has to be on the order
Sheet, 0.25–6.35 mmAMS 4308BStandard product — chemistry, state and mechanical values are fixed by the specification
Plate over 6.35 mmNo AMS coverageChemistry limits and mechanical values stated on the order
Bar and rodNo AMS coverageChemistry limits and mechanical values stated on the order
Extrusion profileNo AMS coverageChemistry, values and section agreed per drawing
TubeNo AMS coverageChemistry, values and dimensions agreed per drawing
Foil and strip below 0.25 mmNo AMS coverageChemistry and values stated on the order

Only the first row has a specification standing behind it. Everything below that line is exactly as good as what the purchase order says, which is why the chemistry and the mechanical values have to be written down instead of referenced.

One more thing to settle before the RFQ goes out: 8009 has no T6 or T8 temper. A T6 or T8 designation means the alloy is hardened by a heat treatment cycle after forming, and this alloy does not harden that way — the particles are already in it and will not re-form. If an offer names T6 or T8 for 8009, the offer is describing a different material.

Two lines on the certificate catch most of the confusion. A zinc figure of 5–6% describes 7075, not 8009, which carries almost no zinc. And a strength figure far above the table above usually means the numbers were carried over from another grade rather than measured on that batch.

We buy 8009 billet, plate and bar from producers that run the powder route, then cut, machine and finish to drawing. For forms outside the AMS range, we quote against the chemistry and the properties your drawing names.

Where 8009 Is Used

Aerospace and Engine-Adjacent Structures

The reason 8009 appears in aerospace work is a weight comparison, not a strength comparison. Above 150 °C the usual alternatives are titanium, steel, and the few heat-resistant aluminiums such as 2618. Titanium is about 50% heavier for the same volume and steel close to three times. A part that can stay aluminium up to 300 °C removes that penalty for anything whose service temperature lands in the band — supersonic airframe skins that heat up in flight, rocket structure, thermal-protection hardware, and brackets and housings close to an engine where the metal soaks up radiant heat without seeing combustion.

The fit is specific rather than general. If the part runs below 150 °C, 7075 or 2024 gives more strength per kilogram and is easier to buy. If it runs above 350 °C, aluminium stops competing and the titanium or steel argument takes over. 8009 earns its place in the band where neither of those answers works.

High-Performance Automotive and Specialty Heat Exchangers

Turbocharger and exhaust-adjacent parts see the same problem in a smaller package: cyclic heating and cooling, with load on the part the whole time. A piston or a housing that softens a little more with every heat cycle loses its clearances before it loses its shape, which is why slow stretching under load at temperature — creep — decides the material here rather than peak strength.

Specialty heat exchangers and high-temperature tooling follow the same logic from the other direction — the part is hot by design, and the question is whether the wall keeps its dimensions over a long campaign. The limiting factor for cost here is usually the size of the part rather than the material: 8009 is expensive relative to 6061, and that premium is easiest to justify on small, highly loaded components.

8009 vs 6061, 2024, 2618 and 7075 — Choosing by Service Temperature

Alloy and temperTensile, room tempYield, room tempPractical service ceilingWhat it is for
7075-T6572 MPa503 MPa~120 °CStrongest at room temperature; wrong choice for a hot part
2024-T3483 MPa345 MPa~150 °CAirframe skins and fatigue-critical structure
6061-T6310 MPa276 MPa~150 °CThe default general-purpose structural alloy
2618-T61~440 MPa~370 MPa~200 °CForged pistons and compressor parts
8009 (H112)450 MPa385 MPa200–300 °CParts that must stay aluminium while running hot
Machined aluminum step block and tensile test specimens illustrating service temperature ceilings from 7075-T6 at 120 °C up to 8009 at 200–300 °C
Practical service temperature ceilings: 8009 uniquely fills the 200–300 °C band before steel or titanium are required.

Room-temperature values above are the minimums published in ASTM B209 for sheet, except 2618, where they are typical forging values to AMS 4132. Service ceilings are practical design limits rather than values printed in any specification, and a specific duty cycle can justify going beyond them with the right testing.

Read that table by the fourth column, not the second. 7075 wins the room-temperature column and is the wrong material for a 250 °C part. 2618 is the right answer for a piston crown at 200 °C and stops being one above it. 8009 is the only grade here with a service ceiling above 200 °C.

That is also why the two alloys are easy to compare the wrong way round. Put the datasheets side by side and 7075 shows 572 MPa against 8009’s 450 MPa, which reads like 8009 is the weaker alloy. It is weaker — at room temperature, on a bench, which is not where the part works.

Working With 8009 — Machining, Joining and Finishing

Machining: it cuts like a hard aluminium, not like 6061. At around 140 HB it behaves much closer to 7075, which means a shop that already runs 7075 will be comfortable and a shop that only runs 6061 should expect faster tool wear and lighter cuts. There is no free-machining version of this alloy, so how the chips break comes down to how the machine is set rather than to the metal.

Joining: welding costs you the property you bought the alloy for. A fusion weld destroys the particle structure in the weld zone, and the joint loses the high-temperature strength that justified the material in the first place. For a load-bearing joint, plan on mechanical fastening, or on a joining method that does not melt the metal and has been qualified for this alloy; treat a fusion-welded joint as non-structural unless it has been tested and accepted on its own.

Comparison between recommended mechanical fastening with countersunk aerospace bolts and prohibited fusion welding showing heat-affected zone cracking on 8009 aluminum
Joining 8009: use mechanical fastening or solid-state methods; conventional fusion welding melts the matrix and destroys dispersoid strength.

Corrosion protection: it holds up well in normal workshop and atmospheric service but it is not a marine alloy. Anodizing works, and so do chemical conversion coatings — a chemical surface treatment that leaves a protective layer on the metal. For a part that will see salt air or chemical exposure, specify the finish on the drawing rather than deciding it after the part is made.

Forming: shape it in O, and accept that you cannot heat-treat the strength back afterwards. This is the biggest practical difference from the 2xxx and 7xxx grades, where forming in a soft state and then aging to full strength is routine. In 8009 the H112 values are set when the material is worked hot, not by a treatment you can repeat in your own shop — so a part that needs heavy forming either starts in O and stays softer, or is formed near-final and machined from H112.

Pros and Limitations at a Glance

DimensionAdvantageWhat it costs
Strength above 200 °CHolds 350 MPa at 200 °C and 270 MPa at 300 °C after 1,000 hoursNothing comparable in the 6xxx or 7xxx families at that temperature
Room-temperature strength450 MPa tensile, comparable to 2618Below 7075 and 2024; not a reason to choose it
Weight2.92 g/cm³ — under half of steel, so it replaces hot steel parts directlyAbout 8% heavier than 6061 for the same volume
Fatigue at temperature160 MPa at 250 °C — published typical value — supports cyclic hot serviceCost per kilogram is several times 6061
MachiningCuts predictably, close to 7075~140 HB wears tooling faster than 6061
JoiningMechanical fastening and methods that do not melt the metal both workFusion welding removes the strength advantage locally
SupplyAvailable as billet, plate and bar from powder-route producersNarrow producer base; lead time follows billet availability; sheet only under AMS 4308
FormingO temper forms wellFormed parts cannot be re-hardened to H112

Conclusion

8009 solves a real problem — carrying load at 200 to 300 °C without moving to titanium or steel — but nothing about it is standard. One producer tier, a specification that covers sheet only, and just two usable states mean the buying problem replaces the engineering problem as soon as the alloy is chosen.

We buy 8009 billet, plate and bar from powder-route producers, then cut and machine to your drawing. Every order ships with an MTC, and SGS reports are available if your project needs them.

Send us the drawing with the form, state and quantity for a supply check and a cutting quote.

Frequently Asked Questions

Can 8009 aluminum be used at 400 °C?

No — there is no published basis for 400 °C. Published 1,000-hour test values, rather than specification minimums, support 200–300 °C; above 350 °C the particle structure needs assessment against your duty cycle.

Does 8009 have a T6 temper?

No. 8009 is strengthened by particles already in the metal, so there is no solution-treat-and-age step to make T6 or T8. It ships in O or H112 only, and an offer naming T6 describes another alloy.

Can you supply 8009 in bar or tube when AMS 4308 covers sheet only?

Yes, as a drawing-controlled item. Outside the AMS thickness range there is no specification to point at, so chemistry and mechanical values travel on the purchase order, and the MTC reports what was tested.

What is the minimum order and lead time for 8009?

Low MOQ, typically 10–60 days. The date depends on billet availability and the cutting or machining you need, so it is confirmed with the quote rather than quoted in advance. Send the drawing, form, state and quantity.

David Huang

David Huang is a highly respected expert in China’s aluminum alloy industry, bringing over a decade of experience in developing, manufacturing, and applying advanced aluminum alloys. He has a proven track record of successfully delivering project solutions and technical expertise to leading global corporations across diverse sectors, including aerospace, automotive, and construction. David also is a trusted advisor to multiple major aluminum manufacturers in China.

24/7 Service | Response Within 10 Minutes!

For more catalogs, details and quotes, please contact us directly!

WhatsApp Phone