Цена на алюминий · 27 ноября 2026 г.
LME $2,983 ▲
SMM A00 $3,455 ▲
Changjiang A00 $3,413 ▲

Алюминиевая сварочная проволока и пруток ER5356

ER5356 aluminum welding filler is an Al-Mg alloy (AlMg5) supplied as MIG spooled wire and TIG straight rod, classified to AWS A5.10 ER5356 and EN ISO 18273 S Al 5356. It delivers high weld strength, good saltwater corrosion resistance and an anodized colour that matches 5xxx base metal — the reason it is the first choice for marine work and for 5xxx-to-6xxx dissimilar joints. Not recommended for continuous service above 65 °C, where the magnesium sensitizes.

Сварочная проволока MIG: 0,8 / 1,0 / 1,2 / 1,6 / 2,0 / 2,4 мм на катушках или в барабанах
Сварочный пруток TIG: 1.6 / 2.4 / 3.2 mm × 914 mm
Base metals: 5052 / 5083 / 5086 / 5454 / 5754, plus 6061 / 6063 / 6082
Документы по качеству: MTC с указанием термической обработки и номера партии

What Is ER5356 Welding Wire & Rod?

ER5356 aluminum welding filler is an Al-Mg alloy (AlMg5, EN AW-AlMg5CrTiMn) for MIG spooled wire and TIG straight rod. It delivers high weld strength, good saltwater corrosion resistance and an anodized colour that matches 5xxx base metal closely, which is why it is the filler for marine and anodized work. It is not recommended for continuous service above 65 °C. Classified to AWS A5.10 ER5356 and EN ISO 18273 S Al 5356. Alloy data: алюминиевый сплав 5356.

Wire or Rod — Forms, Diameters & Packaging

As with 4043, the two names are the same alloy in different delivery forms. Сварочная проволока is continuous and spooled for MIG; сварочный пруток is cut to straight lengths for hand-fed TIG.

Форма Диаметры (мм) Упаковка Типичное применение
Сварочная проволока MIG (на катушках) 0.8, 1.0, 1.2, 1.6, 2.0, 2.4 Стандартные катушки или барабаны Производственная сварка, полуавтоматическая и роботизированная
Сварочный пруток TIG (нарезанный прямыми отрезками) 1.6, 2.4, 3.2 914 mm length Ручная TIG-сварка, ремонтные работы, малые сборки

Со склада или под заказ. Not every diameter is held at all times. Anything in stock ships directly with no minimum order quantity; the rest is produced or sourced to order with a MOQ. Tell us the process, diameter and quantity and we will confirm which applies.

Base Metals

Основной металл Пригодность к обработке Обоснование
5052, 5083, 5086, 5454, 5754 (5xxx) First choice Matches the magnesium level, so strength and corrosion resistance carry through the joint
6061, 6063, 6082 (6xxx) Works well Higher joint strength than 4043, and the weld anodizes close to the base metal
5xxx welded to 6xxx (dissimilar) The standard answer Handles the magnesium mismatch better than any 4xxx filler
Литейный алюминий A356 / A357 Possible, but 4043 is usually better Castings are silicon-based; a silicon filler matches them more closely

If the assembly mixes 5xxx and 6xxx — a 5083 hull with a 6061 frame — 5356 is the filler to specify: the one grade that works on both sides without a strength penalty.

The 65 °C Limit

This is the constraint that decides whether 5356 is the right filler at all, and it is routinely missed.

5356 carries 4.5–5.5% magnesium. In continuous service above roughly 65 °C, that magnesium migrates to the grain boundaries and precipitates as a beta phase. The weld sensitizes: resistance to intergranular corrosion and stress-corrosion cracking drops, silently — nothing about the part changes visibly. The risk is highest in the applications 5356 is bought for, because marine and tank work combines moisture with heat.

Практическое правило: for continuous service above 65 °C, do not specify 5356. Move to a silicon-based filler such as 4043, or tell us the service temperature and medium and we will advise. Intermittent excursions are less critical than sustained temperature, but they still belong in the enquiry rather than being discovered later.

4043 vs 5356 — the One Comparison Everyone Asks

Недвижимость ER4043 (Al-Si 5%) ER5356 (Al-Mg 5%)
Filler type Aluminium-silicon Aluminium-magnesium
Best base metals 6xxx and cast aluminium 5xxx, and 5xxx-to-6xxx dissimilar joints
Flow and wetting Better — more fluid, more forgiving of gaps Less fluid; needs tighter fit-up
Прочность сварного шва Lower (roughly 170–190 MPa deposit) Выше
Saltwater corrosion Умеренный Good — the reason it dominates marine work
Anodized colour Weld zone turns dark grey to black Matches 5xxx base metal closely
Service above 65 °C Acceptable Not recommended — sensitizes

One line: 4043 is the silicon filler for 6xxx and castings — easy-flowing but dark after anodizing. 5356 is the magnesium filler for 5xxx and mixed joints — stronger, salt-water resistant, matching anodized colour, but with a temperature ceiling. Product detail on the other side of the choice: алюминиевый сплав 4043.

Composition & Deposit Properties

Элемент Технические характеристики Элемент Технические характеристики
Магний (Mg) 4.5 - 5.5 Марганец (Mn) 0.05 - 0.20
Хром (Cr) 0.05 - 0.20 Титан (Ti) 0.06 - 0.20
Кремний (Si) 0,25 макс. Железо (Fe) 0,40 макс.
Медь (Cu) 0.10 макс. Цинк (Zn) 0.10 макс.

Weight percent; aluminum is the balance. The chromium and titanium are there to control grain structure and improve as-cast toughness in the weld.

Недвижимость Значение
Tensile strength, filler deposit Higher than 4043 — the reason it is specified where the joint must carry load
Анодированное покрытие Clear to slightly grey, close to 5xxx base metal
Плотность 2,66 г/см³

Wrought 5356 in O and H22 runs 290–320 MPa tensile — higher than most 6xxx base metals, so the joint is usually limited by the base metal, not the filler.

Welding Practice & Applications

Практика: remove oxide and contamination first; aluminium oxide melts far above the metal and causes both porosity and lack of fusion. 5356 is less fluid than 4043, so fit-up matters — a joint that would close up with 4043 may need a groove or a second pass. Use AC TIG or DCEP MIG with pure argon or argon-helium, and do not preheat more than the section needs. Store spools dry — magnesium-bearing wire picks up moisture more readily than silicon wire.

Приложения: boat hulls, decks and superstructures; marine equipment and offshore fittings; RV and truck chassis frames; storage tanks and pressure vessels; bicycle and motorcycle frames; aluminium scaffolding and piping; anodized weldments where the weld must not show; repair of 5xxx structures.

Документы качества и прослеживаемость партий

Каждый заказ отгружается с MTC, выданным Linsy после производства, с указанием обозначения сплава, номера плавки и партии, химического состава, механических результатов и проверки соответствия размеров. На присадочном металле номер партии is what lets you trace a weld back to a coil if a joint fails or a certificate is challenged.

Укажите AWS A5.10 или EN ISO 18273 в запросе, и сертификат будет выдан в соответствии с этой классификацией. Сторонние испытания доступны по запросу за дополнительную плату. Производство осуществляется в рамках систем, сертифицированных по ISO 9001, ISO 14001 и ISO 45001.

Как указать и запросить предложение

  1. Форма — MIG spool wire or TIG cut rod
  2. Диаметр — and the spool or pack weight your process accepts
  3. Количество — spools, tubes or kilograms
  4. Основной металл — including whether the joint is dissimilar 5xxx to 6xxx
  5. Service conditions — operating temperature and medium; above 65 °C sustained, we will steer you to another filler
  6. Отделка после сварки — if the part will not be anodized, 4043 may be the cheaper correct answer
  7. Certification and destination — AWS A5.10 or EN ISO 18273, discharge port and marking

Отдел продаж подтверждает наличие на складе или срок изготовления на заказ для данной конкретной комбинации.

Почему стоит выбрать Linsy

Shenzhen-based aluminum factory, more than 20 years in the industry, supplying 1000–8000 series alloys in standard specifications and custom sizes.

  • MTC с номером плавки и партии на каждый заказ, для прослеживаемости сварки
  • ER5356 MIG spool wire and TIG cut rod, with 4043 as the silicon alternate
  • Low-MOQ custom production, typical custom lead time 10–60 days
  • Technical check on base metal combination and service temperature before the order is accepted
  • Тестирование SGS по запросу; смешанные по спецификациям и проектным заказам обрабатываются как один заказ

Связанные ресурсы

ER5356 Welding Wire & Rod FAQ

Q: What is the difference between ER5356 welding wire and welding rod?
A: Delivery form and process only. Wire is spooled and continuous for MIG; rod is cut to straight lengths for TIG. Both are ER5356.

Q: Can 5356 be used above 65 °C?
A: Not for continuous service. The magnesium sensitizes above that temperature and corrosion resistance drops without any visible change. Tell us the service temperature and we will recommend an alternative filler.

Q: Can 5356 weld 6061?
A: Yes, and with higher joint strength than 4043. The trade-off is that 5356 is less fluid, so fit-up must be tighter. Where the part is not anodized and the joint geometry is awkward, 4043 is often the easier weld.

Q: Why does my anodized weld look better with 5356 than with 4043?
A: Because 5356 is a magnesium filler and matches 5xxx and 6xxx base metal closely, while the silicon in 4043 anodizes dark grey to black. If the weld will be visible after anodizing, 5356 is the correct choice.

Q: Do you supply both wire and rod in the same order?
A: Yes — diameters and forms can be combined into one shipment, and specifications can be mixed with 4043 if you run both processes.

Производственное оборудование

Сертификаты

Склад и запасы

Процесс заказа

Преимущества Linsy

Linsy Aluminum - ведущий поставщик продукции для обработки алюминия, обслуживающий различные отрасли промышленности, включая аэрокосмическую, общее машиностроение, автомобильную, морскую, судостроительную и другие специализированные промышленные приложения.

Мы стремимся поддерживать самые высокие стандарты качества и экологической ответственности, о чем свидетельствуют наши сертификаты: ISO 9001:2008, ISO 14001:2004 и SGS.

Подпишитесь на форму сегодня! Откройте для себя алюминиевые решения премиум-класса с помощью Linsy Alu.