2618 aluminum bar is a heat-treatable Al-Cu-Mg-Ni alloy (EN AW-2618 / AlCu2Mg1.5Ni, UNS A92618) for parts that stay strong when hot — pistons, compressor rotors and high-temperature structural parts. Round bar is supplied from 10 mm to 500 mm; square and flat bar on request. The standard temper is T61, not T6: it is aged at a higher temperature so the material does not over-age and soften in service at 150–250 °C.
Formes : round bar 10–500 mm; square / flat on request; length 1000–6000 mm
Revenus : T61 / T6511 / T4 / T4511 / O
Documents relatifs à la qualité : Rapport MTC joint à chaque commande
2618 is a heat-treatable Al-Cu-Mg-Ni alloy (EN AW-2618 / AlCu2Mg1.5Ni, UNS A92618) used for parts that stay strong when hot — pistons, compressor rotors and high-temperature structural parts. Its deliberate iron and nickel content forms a dispersion that resists coarsening, which is why it holds strength to roughly 250 °C where ordinary age-hardening alloys have already over-aged. Bar is supplied as extruded round bar; the standard temper is T61, not T6. Metallurgy and equivalents: Alliage d'aluminium 2618.
Round bar is the form we hold and quote most often. Square and flat bar are available on request against your section.
| Formulaire | Diameter / side (mm) | Longueur (mm) | Disponibilité |
|---|---|---|---|
| Barre ronde, extrudée | 10 – 500 | 1000 – 6000 (coupé à longueur) | Standard range |
| Barre carrée | Quoted to section | 1000 – 6000 | Sur demande |
| Barre plate | Quoted to section | 1000 – 6000 | Sur demande |
Other 2618 forms — sheet, plate, tube, forging stock and wire — are described on the page de l'alliage. For bar in other alloys, see the gamme de barres en aluminium.
| Tempérer | État | Résistance à la traction (MPa) | Limite d'élasticité (MPa) | Élongation | À spécifier pour |
|---|---|---|---|---|---|
| T61 | Solution treated, artificially aged at elevated temperature | ≥ 400 | ≥ 310 | ~8% | The standard for 2618: pistons, hot tooling, heat-exposed structure |
| T6511 | As T61, stress relieved by stretching and straightened | ≥ 400 | ≥ 310 | ~8% | Precision machining of bar where the part must not move |
| T4 / T4511 | Mis en solution, vieilli naturellement | Selon le MTC | Bar formed after delivery; low enquiry volume | ||
| O | Recuit | ~200 | ~100 | ~14% | Machining stock before ageing, forming |
Values are typical for 2618 and confirmed against the MTC for the lot. Hardness is roughly 115 HB in T61 and 55 HB in O. Density 2.70 g/cm³.
On 6061 or 6082 the default is T6. On 2618 it is T61, and the difference is the ageing temperature, not an extra process step. T61 is aged at a higher temperature than a standard T6, which deliberately over-ages the alloy slightly: peak room-temperature strength is traded for stability, so the material does not continue to over-age and soften in service at 150–250 °C. That is exactly the range pistons and hot tooling live in.
Practical consequence: if a drawing for a piston or hot fixture specifies 2618-T6, question it. T6 can be quoted, but it is rarely what the application needs and it is not the temper the industry writes on 2618. T6511 is the same T61 condition with the bar stretched after quenching and then straightened — strength unchanged, residual stress removed, so long machined parts stay straight.
The same designation rule as other extrusions applies: T651 is rolled plate, not bar. Extruded bar is stress relieved as T6511. A bar certificate showing T651 is a designation error.
En stock ou sur commande. Ces revenus ne sont pas tous détenus dans chaque épaisseur et section. Une combinaison en stock est expédiée directement, sans quantité minimale de commande. Comme la plage de revenus est large, le reste est produit sur commande avec une MOQ — indiquez-nous le revenu, la dimension et la quantité et nous confirmerons ce qui s'applique et vous fournirons un devis.
| Élément | Spécifications | Élément | Spécifications |
|---|---|---|---|
| Cuivre (Cu) | 1.9 – 2.7 | Magnésium (Mg) | 1.3 – 1.8 |
| Nickel (Ni) | 0.9 – 1.2 | Fer (Fe) | 0.9 – 1.3 |
| Silicium (Si) | 0.10 – 0.25 | Titane (Ti) | 0.04 – 0.10 |
| Manganèse (Mn) | 0,15 max | Chrome (Cr) | 0,10 max |
| Zinc (Zn) | 0,15 max | Autres, chacun / total | 0.05 / 0.15 |
Weight percent; aluminum is the balance. The nickel and iron are intentional, not impurities — they form the intermetallic dispersion that gives 2618 its hot strength.
Engine pistons and piston crowns, compressor impellers and rotors, high-temperature structural brackets, helicopter rotor components, plastic injection moulds and hot fixtures, automotive connecting rods and other engine parts machined to tight tolerance. For the other common piston alloy, see Alliage d'aluminium 4032.
Two limits belong on the enquiry rather than in the workshop:
Every order ships with an MTC issued by Linsy after production, reporting composition, mechanical results and the temper designation. Third-party testing is available on request at additional cost. Production runs under ISO 9001, ISO 14001 and ISO 45001 certified systems.
Le service commercial confirme le stock ou le délai de fabrication sur mesure pour cette combinaison exacte.
Shenzhen-based aluminum factory, more than 20 years in the industry, supplying 1000–8000 series alloys in standard specifications and custom sizes. 2618 round bar in T61 and T6511, with square and flat sections quoted on request; MTC with every order; low-MOQ custom production; typical custom lead time 10–60 days.
Q: Do you supply 2618 bar in T6?
A: T6 can be quoted, but it is rarely what a 2618 application needs and it is not the temper the industry specifies. T61 is aged at a higher temperature specifically so the part keeps its strength at 150–250 °C. If your drawing says 2618-T6, tell us the service temperature and we will confirm what to order.
Q: Can you supply square or flat 2618 bar?
A: On request. Round bar from 10 mm to 500 mm is the standard range; square and flat sections are quoted to your dimensions and quantity. Send the section, length and quantity.
Q: Is T6511 different from T61 in strength?
A: No — both are ≥400 MPa tensile and ≥310 MPa yield. T6511 is stretched after quenching to remove residual stress and then straightened, so long machined parts do not move. Choose it for precision machining, T61 for everything else.
Q: Can 2618 bar be welded?
A: Fusion welding is not recommended — the copper content causes hot cracking in TIG and MIG. Mechanical fastening or press-fit is the usual route for assembly.