Precio del aluminio · 27 de noviembre de 2026
LME $2,983 ▲
SMM A00 $3,455 ▲
Changjiang A00 $3,413 ▲

ER5356 Aluminum Welding Wire & Rod

ER5356 aluminum welding filler is an Al-Mg alloy (AlMg5) supplied as MIG spooled wire and TIG straight rod, classified to AWS A5.10 ER5356 and EN ISO 18273 S Al 5356. It delivers high weld strength, good saltwater corrosion resistance and an anodized colour that matches 5xxx base metal — the reason it is the first choice for marine work and for 5xxx-to-6xxx dissimilar joints. Not recommended for continuous service above 65 °C, where the magnesium sensitizes.

MIG welding wire: 0.8 / 1.0 / 1.2 / 1.6 / 2.0 / 2.4 mm spools or drums
TIG welding rod: 1.6 / 2.4 / 3.2 mm × 914 mm
Base metals: 5052 / 5083 / 5086 / 5454 / 5754, plus 6061 / 6063 / 6082
Documentos de calidad: MTC with heat and lot number

What Is ER5356 Welding Wire & Rod?

ER5356 aluminum welding filler is an Al-Mg alloy (AlMg5, EN AW-AlMg5CrTiMn) for MIG spooled wire and TIG straight rod. It delivers high weld strength, good saltwater corrosion resistance and an anodized colour that matches 5xxx base metal closely, which is why it is the filler for marine and anodized work. It is not recommended for continuous service above 65 °C. Classified to AWS A5.10 ER5356 and EN ISO 18273 S Al 5356. Alloy data: Aleación de aluminio 5356.

Wire or Rod — Forms, Diameters & Packaging

As with 4043, the two names are the same alloy in different delivery forms. Welding wire is continuous and spooled for MIG; welding rod is cut to straight lengths for hand-fed TIG.

Formulario Diameters (mm) Embalaje Uso típico
MIG welding wire (spooled) 0.8, 1.0, 1.2, 1.6, 2.0, 2.4 Standard spools or drums Production welding, semi-automatic and robotic
TIG welding rod (straight cut) 1.6, 2.4, 3.2 914 mm length Manual TIG, repair work, small assemblies

De stock o fabricado bajo pedido. Not every diameter is held at all times. Anything in stock ships directly with no minimum order quantity; the rest is produced or sourced to order with a MOQ. Tell us the process, diameter and quantity and we will confirm which applies.

Base Metals

Metal común Idoneidad Por qué
5052, 5083, 5086, 5454, 5754 (5xxx) First choice Matches the magnesium level, so strength and corrosion resistance carry through the joint
6061, 6063, 6082 (6xxx) Works well Higher joint strength than 4043, and the weld anodizes close to the base metal
5xxx welded to 6xxx (dissimilar) The standard answer Handles the magnesium mismatch better than any 4xxx filler
Cast aluminium A356 / A357 Possible, but 4043 is usually better Castings are silicon-based; a silicon filler matches them more closely

If the assembly mixes 5xxx and 6xxx — a 5083 hull with a 6061 frame — 5356 is the filler to specify: the one grade that works on both sides without a strength penalty.

The 65 °C Limit

This is the constraint that decides whether 5356 is the right filler at all, and it is routinely missed.

5356 carries 4.5–5.5% magnesium. In continuous service above roughly 65 °C, that magnesium migrates to the grain boundaries and precipitates as a beta phase. The weld sensitizes: resistance to intergranular corrosion and stress-corrosion cracking drops, silently — nothing about the part changes visibly. The risk is highest in the applications 5356 is bought for, because marine and tank work combines moisture with heat.

Regla práctica: for continuous service above 65 °C, do not specify 5356. Move to a silicon-based filler such as 4043, or tell us the service temperature and medium and we will advise. Intermittent excursions are less critical than sustained temperature, but they still belong in the enquiry rather than being discovered later.

4043 vs 5356 — the One Comparison Everyone Asks

Propiedad ER4043 (Al-Si 5%) ER5356 (Al-Mg 5%)
Filler type Aluminium-silicon Aluminium-magnesium
Best base metals 6xxx and cast aluminium 5xxx, and 5xxx-to-6xxx dissimilar joints
Flow and wetting Better — more fluid, more forgiving of gaps Less fluid; needs tighter fit-up
Weld strength Lower (roughly 170–190 MPa deposit) Más alto
Saltwater corrosion Moderado Good — the reason it dominates marine work
Anodized colour Weld zone turns dark grey to black Matches 5xxx base metal closely
Service above 65 °C Acceptable Not recommended — sensitizes

One line: 4043 is the silicon filler for 6xxx and castings — easy-flowing but dark after anodizing. 5356 is the magnesium filler for 5xxx and mixed joints — stronger, salt-water resistant, matching anodized colour, but with a temperature ceiling. Product detail on the other side of the choice: Aleación de aluminio 4043.

Composition & Deposit Properties

Elemento Especificación Elemento Especificación
Magnesio (Mg) 4.5 - 5.5 Manganeso (Mn) 0.05 - 0.20
Cromo (Cr) 0.05 - 0.20 Titanio (Ti) 0.06 - 0.20
Silicio (Si) 0,25 máx. Hierro (Fe) 0.40 máx.
Cobre (Cu) 0,10 máx. Zinc (Zn) 0,10 máx.

Weight percent; aluminum is the balance. The chromium and titanium are there to control grain structure and improve as-cast toughness in the weld.

Propiedad Valor
Tensile strength, filler deposit Higher than 4043 — the reason it is specified where the joint must carry load
Acabado anodizado Clear to slightly grey, close to 5xxx base metal
Densidad 2,66 g/cm³

Wrought 5356 in O and H22 runs 290–320 MPa tensile — higher than most 6xxx base metals, so the joint is usually limited by the base metal, not the filler.

Welding Practice & Applications

Practice: remove oxide and contamination first; aluminium oxide melts far above the metal and causes both porosity and lack of fusion. 5356 is less fluid than 4043, so fit-up matters — a joint that would close up with 4043 may need a groove or a second pass. Use AC TIG or DCEP MIG with pure argon or argon-helium, and do not preheat more than the section needs. Store spools dry — magnesium-bearing wire picks up moisture more readily than silicon wire.

Aplicaciones: boat hulls, decks and superstructures; marine equipment and offshore fittings; RV and truck chassis frames; storage tanks and pressure vessels; bicycle and motorcycle frames; aluminium scaffolding and piping; anodized weldments where the weld must not show; repair of 5xxx structures.

Quality Documents & Lot Traceability

Every order ships with an MTC issued by Linsy after production, reporting the alloy designation, heat and lot number, chemical composition, mechanical results and a dimensional conformance check. On filler metal the lot number is what lets you trace a weld back to a coil if a joint fails or a certificate is challenged.

State AWS A5.10 or EN ISO 18273 on the enquiry and the certificate is issued against that classification. Third-party testing is available on request at additional cost. Production runs under ISO 9001, ISO 14001 and ISO 45001 certified systems.

Cómo especificar y solicitar cotización

  1. Formulario — MIG spool wire or TIG cut rod
  2. Diámetro — and the spool or pack weight your process accepts
  3. Cantidad — spools, tubes or kilograms
  4. Metal común — including whether the joint is dissimilar 5xxx to 6xxx
  5. Service conditions — operating temperature and medium; above 65 °C sustained, we will steer you to another filler
  6. Post-weld finish — if the part will not be anodized, 4043 may be the cheaper correct answer
  7. Certification and destination — AWS A5.10 or EN ISO 18273, discharge port and marking

Ventas confirma stock o plazo de entrega personalizado para esa combinación exacta.

Por qué elegir Linsy

Shenzhen-based aluminum factory, more than 20 years in the industry, supplying 1000–8000 series alloys in standard specifications and custom sizes.

  • MTC with heat and lot number on every order, for weld traceability
  • ER5356 MIG spool wire and TIG cut rod, with 4043 as the silicon alternate
  • Low-MOQ custom production, typical custom lead time 10–60 days
  • Technical check on base metal combination and service temperature before the order is accepted
  • Ensayos SGS a solicitud; pedidos de especificaciones mixtas y de proyecto gestionados como un solo pedido

Recursos relacionados

ER5356 Welding Wire & Rod FAQ

Q: What is the difference between ER5356 welding wire and welding rod?
A: Delivery form and process only. Wire is spooled and continuous for MIG; rod is cut to straight lengths for TIG. Both are ER5356.

Q: Can 5356 be used above 65 °C?
A: Not for continuous service. The magnesium sensitizes above that temperature and corrosion resistance drops without any visible change. Tell us the service temperature and we will recommend an alternative filler.

Q: Can 5356 weld 6061?
A: Yes, and with higher joint strength than 4043. The trade-off is that 5356 is less fluid, so fit-up must be tighter. Where the part is not anodized and the joint geometry is awkward, 4043 is often the easier weld.

Q: Why does my anodized weld look better with 5356 than with 4043?
A: Because 5356 is a magnesium filler and matches 5xxx and 6xxx base metal closely, while the silicon in 4043 anodizes dark grey to black. If the weld will be visible after anodizing, 5356 is the correct choice.

Q: Do you supply both wire and rod in the same order?
A: Yes — diameters and forms can be combined into one shipment, and specifications can be mixed with 4043 if you run both processes.

Equipos de producción

Certificaciones

Almacén y existencias

Proceso de pedido

Ventajas de Linsy

Linsy Aluminum es un proveedor líder de productos de procesamiento de aluminio, que presta servicio a diversas industrias, como la aeroespacial, la ingeniería general, la automoción, la marina, la construcción naval y otras aplicaciones industriales especializadas.

Nos comprometemos a mantener los más altos estándares de calidad y responsabilidad medioambiental, como demuestran nuestras certificaciones: ISO 9001:2008, ISO 14001:2004 y SGS.

¡INSCRÍBETE en el formulario hoy mismo! Descubra sus soluciones de aluminio de primera calidad con Linsy Alu.